836 鋼の疲労強度に及ぼす WPC 処理による表面粗さの影響
スポンサーリンク
概要
- 論文の詳細を見る
This study was carried out to improve the fatigue strength of steel with many surface modifications. Wide Peaning Cleaning (WPC) process was developed recently. Three factors of high hardness, high compressive residual stress and deterioration of suface roughness are added on surface layer with WPC process, and it is said that these factors will define the fatigue strength. We estimated quantitately the effect upon the fatigue strength by these factors. Furthemore we presumed and verified the presence of the maximum size of dent that influences the fatigue strength. The analysis resuts were almost accordance with the experimental result and it is shown that the prediction of fatigue strength of the steel modified with WPC process.
- 社団法人日本機械学会の論文
- 2000-07-31
著者
-
米倉 大介
徳島大学工学部機械工学科
-
曙 紘之
広島大学工学部
-
清水 真佐男
慶應義塾大学理工学部
-
曙 紘之
慶大院
-
清水 真佐男
慶大
-
小茂鳥 潤
慶大
-
清水 真佐男
慶應大
-
小茂鳥 潤
慶大・理工
-
宮坂 四志男
株式会社不二機販
-
米倉 大介
徳島大学 工学部
-
野田 淳二
慶大院
-
宮坂 四志男
不二機販
-
米倉 大介
徳島大・工
関連論文
- シリカ粉体の付着・堆積挙動に及ぼす鋼板表面研磨処理の影響(機械要素,潤滑,設計,生産加工,生産システムなど)
- 高疲労特性を有する自溶合金溶射部材作製のための有効な再溶融処理方法の提案(ガスタービン用遮熱/耐環境コーティング技術)
- 自溶合金溶射部材の疲労強度に及ぼす基材表面粗さの影響
- 自溶合金溶射部材の疲労特性に及ぼす基材表面粗さの影響(S14-1 溶射材の疲労,S14 金属材料の疲労特性と破壊機構)
- 自溶合金溶射部材の疲労特性に及ぼす再溶融処理時間の影響
- 1131 自溶合金溶射部材の疲労特性に及ぼす表面形状の影響
- 1129 自溶合金溶射部材の疲労特性に及ぼす拡散層の影響
- 1128 溶射部材の疲労特性に及ぼす再溶融処理時間の影響
- 827 異なる界面密着強度を有する溶射部材の疲労特性に及ぼす界面拡散層の影響
- 812 マイクロ波プラズマCVD法により作製したダイヤモンド薄膜の化学修飾(表面改質・色彩評価,一般セッション,第53期学術講演会)