軟鋼およびHT60の切欠広幅継手の低サイクル疲労特性
スポンサーリンク
概要
- 論文の詳細を見る
Welded and notched wide plate specimens of high tensile structural steel were tested in constant load tests and constant net section stress tests, and welded and notched wide plate specimens and notched wide plate specimens of mild steel were also tested in constant load tests.In each series three of initial notch lengths were provided in order to determine the effect of material properties at notch root ; mother metal, heat affected zone and deposited metal.As a result of the tests it was found that the material properties at notch root and residual stress influcence very little the initiation and propagation behavior of the low cycle fatigue crack, if weldment matches mother metal well, and that fatigue crack propagation rate changes in accordance with the change of the mode of fatigue crack.
- 社団法人日本船舶海洋工学会の論文
著者
関連論文
- (45) 低荷重脆性破壊の発生に及ぼす低サイクル疲労履歴の影響
- (41) 切欠先端の靱性および歪履歴が脆性破壊発生限界曲線に及ぼず影響
- レインフロウ法の考え方とその応用 : 疲労の累積被害評価法
- 海洋構造物用重防食塗膜の膜圧分布(氷海技術部,所外発表論文等概要)
- 478 海洋構造物用重防食塗装の膜厚分布(海洋構造物の腐食と防食・破壊と疲労, 加工・システム・利用技術, 日本鉄鋼協会第 112 回(秋季)講演大会)
- 熱冷衝撃法を用いた海洋構造物用重防食塗膜の評価(船体構造部,所外発表論文等概要)
- 第 4 回原子力における非破壊検査の国際会議
- 第 XIII 委員会出席報告 : Fatigue Testing(1972 年 IIW 年次大会(トロント)出席報告)
- 第 XIII 委員会出席報告 : Fatigue Testing(1971 年 IIW 年次大会(ストックホルム)出席報告)
- 総合報告(1971 年 IIW 年次大会(ストックホルム)出席報告)