Synthesis of Diamond-like Carbon Films by Nanopulse Plasma Chemical Vapor Deposition at Subatmospheric Pressure
スポンサーリンク
概要
- 論文の詳細を見る
The deposition of diamond-like carbon (DLC) films at subatmospheric pressure has been achieved by the nanopulse plasma chemical vapor deposition (CVD) method. To realize this process, a high ion density and non-arcing plasma at subatmospheric pressure are required. A static induction (SI) thyristor with an inductive energy storage (IES) circuit was used. The DLC film was obtained under the conventional low-pressure process at 6 Pa, and the characteristics of the high electron temperature and the exponential relationship between pulse frequency and growth rate were observed. Deposition of the DLC film was also achieved at the subatmospheric pressure of 26.7 kPa (200 Torr) using this nanopulse plasma CVD method.
- INSTITUTE OF PURE AND APPLIED PHYSICSの論文
- 2004-11-01
著者
-
Ohtake Naoto
Department Of Anatomy Shinshu University School Of Medicine
-
Kondo Yoshimasa
Ngk Insulators Ltd.
-
IMANISHI Yu-ichiro
NGK Insulators
-
Hosono Shintaro
Department Of Mechanical Sciences And Engineering Tokyo Institute Of Technology
-
Saito Takao
Ngk Insulators Ltd.
-
NAKAMURA Yukinori
NGK Insulators
-
Kondo Yoshimasa
NGK Insulators, 2-56 Suda, Mizuho-ku, Nagoya 467-8530, Japan
関連論文
- HISTOCHEMICAL STUDIES ON PEROXISOMES OF RAT LIVERS DURING DEHP ADMINISTRATION AND AFTER WITHDRAWAL ON THICK SECTIONS BY MEANS OF LIGHT MICROSCOPY AND HIGH VOLTAGE ELECTRON MICROSCOPY
- Immunocytochemical Study on Intracellular Localization of M protein in Vesicular Stomatitis Virus (VSV)
- Size Dependence of Morphology of Diamond Surfaces Prepared by DC Arc Plasma Jet Chemical Vapor Deposition
- B-12 Rapid Growth of Diamond-like Carbon Films by Nanopulse Magnetron Chemical Vapor Deposition(Session: Coatings/Thin Films)
- Effect of Filler Orientation on Thermal Conductivity of Polypropylene Matrix Carbon Nanofiber Composites
- Structure and Mechanical Properties of Diamond-Like Carbon Films Prepared from C2H2 and H2 Mixtures by Pulse Plasma Chemical Vapor Deposition
- Synthesis of Diamond-like Carbon Films by Nanopulse Plasma Chemical Vapor Deposition at Subatmospheric Pressure
- Wear Resistance of Microextrusion Dies Coated by Diamond-Like Carbon Films
- 405 Wear Resistance of Microextrusion Dies Coated by Diamond-like Carbon Films
- Effect of Filler Orientation on Thermal Conductivity of Polypropylene Matrix Carbon Nanofiber Composites
- Effects of Oxygen Addition on Growth of Diamond Film by Arc Discharge Plasma Jet Chemical Vapor Deposition
- Balloon Cell Melanoma Cells in Metastatic Lesions from Pedunculated Malignant Melanoma
- Synthesis of Diamond-Like Carbon Films by Nanopulse Plasma Chemical Vapor Deposition in Open Air
- OS11(1)-3(OS11W0383) Non-Propagating Crack at Ultra High Cycle Fretting Fatigue Limit
- Effect of Understress on Fretting Fatigue Crack Initiation of Press-Fitted Axle
- 127 Effect of Under Stress on Fretting Fatigue Crack Initiation of Press-Fitted Axle
- Injection Molding of Polystyrene Matrix Composites Filled with Vapor Grown Carbon Fiber
- 227 Injection Molding of Polystyrene Matrix Composites Filled with Vapor Grown Carbon Fiber
- 636 Transcription Mechanism of Minute Surface Pattern in Injection Molding
- Rapid Growth of Diamond-like Carbon Films by Nanopulse Magnetron Chemical Vapor Deposition
- Synthesis and Characterization of Zinc-Doped Amorphous Carbon Films by Plasma-Assisted Organometallic Chemical Vapor Deposition
- Correlation between Optical Properties and Hardness of Diamond-Like Carbon Films
- Synthesis of Diamond-Like Carbon Films by Nanopulse Plasma Chemical Vapor Deposition in Open Air
- Synthesis of Diamond-like Carbon Films by Nanopulse Plasma Chemical Vapor Deposition at Subatmospheric Pressure