熱影響部の脆化について(第 7 報) : 綜合衝撃法による低温脆性の研究
スポンサーリンク
概要
- 論文の詳細を見る
To investigate the weldabilities of Killed and Rimmed steels, using the electrodes of the types of both Low-Hydrogen and Ilmenite the low temperature-brittle ness tests are carried out by the "Synthetic Impact Test Method. As the effect of the electrodes for the weldabilities it was recognized that Low-hydrogen type is superior than Ilmenite, but, in the temperature range lower than -20℃, there is no differenses in the impact values. As the effects of the steels types, Killed steel is excellent, but no differenses lower than 0℃. So that there exist no differenses in the point of impact values, at the temperatures lower than -20℃., in spite of the types of the electrodes and the kinds of the steels, and these phenomena will, mainly, depend upon the mechanisms of the crack propagations, which initiates in the heat-affected parent plates. Transition zone of the rimmed steel is wider than killed, and the first sign of the brittleness is higher temperature than killed.
- 1956-05-25
著者
関連論文
- 放射性同位元素 S^ による研究(第 2 報) : 母材 S の熔着金属えの拡散について
- 放射性同位元素 S^ による研究(第 1 報)
- 熱影響部の脆化について(第 5 報) : 補遺綜合衝撃試驗片の幅の効果
- 軟鋼熔着金属中の Mo と低温脆性
- 熱影響部の脆化について(第 4 報) : 低温脆性について
- 熱影響部の脆化について(第 3 報) : 低水素型及びイルミナイト型の衝撃値分布
- 熱影響部の脆化について(第 2 報) : Single Bead による脆化
- 熱影響部の脆化について(第 1 報) : キルド鋼, リムド鋼の熱処理効果
- 熱影響部の脆化について(第 7 報) : 綜合衝撃法による低温脆性の研究
- 熱影響部の脆化について(第 5 報) : 綜合衝撃試驗法について
- 1 溶接部のミクロ的な不均一性と継手の強度
- Cuの凍結空孔 : 格子欠陥
- 4a-E-1 溶着鋼中の酸化介在物に関するX線的研究
- 多層熔接部の脆化, 熱処理による回復(その 2)
- 熱影響部の脆化について(第 6 報) : 多層熔接部の脆化, 熱処理による回復(その 1)
- deep fillet 熔接棒 (II)
- Deep Fillet 熔接棒 (I)
- 曲げ試験について
- 熔接部の窒素に関する物理的研究(第 1 報)
- 軟鋼熔接部の活性化エネルギーについて(第 2 報)
- 軟鋼熔接部の活性化エネルギーについて (I)
- 8. 軟鋼熔接部の活性化エネルギーについて