バインダー用ゴムを用いた異方性磁性粉末の圧延加工
スポンサーリンク
概要
- 論文の詳細を見る
A magnetic composite material is fabricated by rolling. Anisotropic strontium ferrite powder, Zn-22Al superplastic powder and synthetic rubber are mixed with various mixing ratio and then kneaded. The kneaded compact is rolled at temparature ranging from 50°C to 120°C. It is investigated with regard to fabrication factors such as rolling reduction, rolling temperature, mixing ratio of ferromagnetic powder and Zn-22Al superplastic one, and addition of calcium stearate on characteristics of the magnetic composite material.<BR>The magnetic comosite material imparts flexibility under load. It is found that the optimum forming conditions are a reduction of approximately 90% and a rolling temperature of 80°C Residual flux density of the magnetic composite material almost reaches the theoretical value for a given ferrite content per unit volume. This means that orientation of the ferromagnetic powder is accomplished almost completely.
著者
-
沖本 邦郎
摂南大学工学部
-
山口 勝
久留米工業大学
-
佐藤 富雄
九州工業技術研究所
-
沖本 邦郎
九州工業技術試験所
-
水江 宏
大分県工業試験場
-
渡部 正之
戸田工業(株)
-
堀石 七生
戸田工業(株)
-
沖本 邦郎
九州工業技術研究所
関連論文
- 粉末の成形と焼結に関する材料試験
- 粉末成形におけるニヤネットシェイプ金型技術
- パーマロイ/ステンレス鋼焼結接合複合材の接合強度に及ぼす造粒粉の影響(複合材料)
- SUS316Lステンレス鋼とFe-47Niパーマロイの圧紛体の組み合わせ焼結接合
- 樹脂を含浸した鉄系焼結体の熱的性質
- 遠心噴霧法による過共晶Al-Si系P/M合金の超塑性特性
- 遠心噴霧法による過共晶Al-Si系P/M合金の超塑性特性(塑性工学)
- 遠心噴霧急冷凝固粉の収率に及ぼす要因 (粉末製造技術)
- AZ31マグネシウム合金切屑を用いたFe_3B/Nd_2Fe_B系メタルボンド磁石
- 308 ろう材用Sn基粉末を用いたNd-Fe-B系ナノコンポジットメタルボンド磁石(ナノコンポジットI, 複合材料の成形・加工最前線)