In a quantometric simultaneous determination of alloyed white cast iron, analytical accuracy of silicon can not easily be made comparable with that of other elements (Mn, Ni, Cr, Mo, V and Mg).Especially, when the silicon content is below 0.7%, some large error is apt to be on the result.To better the accuracy of silicon analysis, excitation condition and effect of metallurgical history of test materials are mainly investigated with the following results.<BR>(1) Reproducibility of result is best by high voltage spark method (power supply: 140V;R: residual;C: 0.007 μF×4;L: 0 μH;counter electrode: tungsten;prespark time: 50 sec.;integration time: 20 sec.).<BR>(2) If residual austenite in micro-structure is decomposed prior to the analysis by heat treatment (550° for 1-3 hrs) of both the standard and the Ctest materials, better accuracy will be obtained.<BR>(3) The line pair Fe 2714 Å/Si 2516 Å gives the best result.
- 社団法人 日本分光学会の論文
著者
関連論文
- 204 ヨードメタノール法による高炭素, クロム鋼中の酸化介在物の定量(分析, 日本鉄鋼協会第 68 回(秋季)講演大会講演論文集 (II))
- 54 メタン内部標準法による炉内雰囲気ガスのガスクロマトグラフ分析(製銑および分析, 日本鉄鋼協会第 66 回(秋季)講演大会講演大要)
- 157 ホット・ストリップ仕上圧延機 1 号, 2 号スタンドにおける完全白鋳鉄ロールの肌荒れについて : ホット・ストリップ仕上圧延機用粗ロールの肌荒れ防止に関する研究 III(性質, 日本鉄鋼協会第 65 回(春季)講演大会講演大要)
- 95 ホットストリップ仕上圧延機 1 号および 2 号スタンド専用ワーク・ロールの材質および溶解条件決定のために行なつた諸実験 : ホットストリップ仕上圧延機用粗ロールの肌荒れ防止に関する研究 II(加工, 日本鉄鋼協会第 64 回(秋季)講演大会講演大要)
- 95 ホットストリップ仕上圧延機 1 号および 2 号スタンド用ロールの肌荒れの実態およびその機構について : ホットストリップ仕上圧延機用粗ロールの肌荒れ防止に関する研究 I(加工, 日本鉄鋼協会第 63 回(春季)講演大会講演大要)
- 鉄鋸の發光分光分析における誤差要図 (第1報)
- カントレコーダーによる白鋳鉄中のケイ素分析について
- 鉄鋼の発光分光分析における誤差要因 (第2報) : 試料温度およびチル試料表面の富化偏析の影響
- Quantometric Analysis of Phosphorus in White Cart Iron