In quantometric analysis, though the cause of error is an important problem, fundamental and systematic studies on this subject have not so far been made.In this regard, the case of rapid quantometric analysis of iron and steel has been taken up to look into the analytical accuracy influenced by sample surface condition and sample setting technique with the results summarized below.<BR>(1) If the sample surface is finished off with #80-#180 emery paper, the error on analytical results will become negligible.The surface had better be finished rough to a certain extent, for a discharge surface of such finish raises the accuracy of result.<BR>(2) When the discharge is over small cracks, the result becomes less erroneous.<BR>(3) If the electrode is so set as a part of the surface near the electrode becomes also a light source.the result will be very much affected by such setting.<BR>(4) The discharge at 6-8mm away from the edge of sample surface gives the best result. On cast samples, because of possible cavities and uneven structure, the result obtained at the central portion of the sample may deviate largely from the mean value.<BR>(5) The difference of ±2° in cone-angles of tungsten electrode does not affect the result.
- 社団法人 日本分光学会の論文
著者
関連論文
- 204 ヨードメタノール法による高炭素, クロム鋼中の酸化介在物の定量(分析, 日本鉄鋼協会第 68 回(秋季)講演大会講演論文集 (II))
- 54 メタン内部標準法による炉内雰囲気ガスのガスクロマトグラフ分析(製銑および分析, 日本鉄鋼協会第 66 回(秋季)講演大会講演大要)
- 157 ホット・ストリップ仕上圧延機 1 号, 2 号スタンドにおける完全白鋳鉄ロールの肌荒れについて : ホット・ストリップ仕上圧延機用粗ロールの肌荒れ防止に関する研究 III(性質, 日本鉄鋼協会第 65 回(春季)講演大会講演大要)
- 95 ホットストリップ仕上圧延機 1 号および 2 号スタンド専用ワーク・ロールの材質および溶解条件決定のために行なつた諸実験 : ホットストリップ仕上圧延機用粗ロールの肌荒れ防止に関する研究 II(加工, 日本鉄鋼協会第 64 回(秋季)講演大会講演大要)
- 95 ホットストリップ仕上圧延機 1 号および 2 号スタンド用ロールの肌荒れの実態およびその機構について : ホットストリップ仕上圧延機用粗ロールの肌荒れ防止に関する研究 I(加工, 日本鉄鋼協会第 63 回(春季)講演大会講演大要)
- 鉄鋸の發光分光分析における誤差要図 (第1報)
- カントレコーダーによる白鋳鉄中のケイ素分析について
- 鉄鋼の発光分光分析における誤差要因 (第2報) : 試料温度およびチル試料表面の富化偏析の影響
- Quantometric Analysis of Phosphorus in White Cart Iron