90゜ベンド内層流の凝固閉そく限界 : 曲円管流の無次元整理に関連して
スポンサーリンク
概要
- 論文の詳細を見る
Experiments on solidification blockage of 90° bend laminar flow were made with two R/a ratio double cylinders. The inner pipe of the cylinder was supplied a developed laminar water flow, and through the outer pipe flowed a low temparature coolant supplied from a reservoir. With the ordinary dimensionless axial coordinate for the straight pipe, two critical curves for blokage were obtained according to the R/a ratios. Available calculated and experimental results were used to see a proper dimensionless axial coordinate which could compactly represent curved pipe flow heat transfer, and ζ^* = (z/R)/Pr^m(De・a_R)^n was selected with m=1 and n=1/2. The two critical curves fall into a single critical curve with the thus derived ζ^*_0 = (z_0/R)/Pr(De・a_R)^<1/2> [u_0 = (π/2)・R for 90゜ bend].
- 一般社団法人日本機械学会の論文
- 1988-01-25
著者
関連論文
- 準安定β型チタン合金の加工に伴う組織と材料特性の変化
- Ti-8mass%Mo合金におけるα"マルテンサイト組織の時効に伴う相変態
- 焼入れ冷却中に現れる相変態熱と鋼の炭素量
- 鋼焼入れの伝熱現象の研究 : 第4報,硬さと焼入れ冷却曲線
- 鋼焼入れの伝熱現象の研究 : 相変態熱について
- 凝固を伴う直円管流の熱伝達実験 : 冷却強さがT^*_w≦10の場合
- 等速冷却における純鉄と炭素鋼の相変態温度および相変態熱の測定
- 層流直円管部を冷却される管路系の凝固閉そく限界
- 凝固を伴う円管内定常層流熱伝達
- 鋼焼入れの伝熱現象の研究 : 第3報,焼入れの際の冷却曲線と過渡沸騰熱伝達
- 焼入れと組織制御研究部会
- チタン合金の昇温に伴う相変態と物性の変化 (特集記事 神大テクノフェスタ2008) -- (大学重要機器整備費による教育・研究成果の報告)
- 鋼のさまざまな直径に対する相変態を伴う冷却曲線の一解析
- 鋼焼入れの伝熱現象の研究 : 第2報,相変態を伴う冷却曲線の一考察
- 焼入れにおける鋼のかたさと冷却水温度の関係〔英文〕
- 425 鉄系合金の相変態熱の測定(金属系材料)
- すばらしき先達に恵まれて
- 鋼のパーライト変態熱に対する炭素およびクロム濃度の影響(相変態・材料組織)
- 鉄鋼の相変態熱に対する炭素濃度の影響
- 水焼入れ中の相変態に対する鋼の炭素量 (0.34〜0.73%)の影響
- 90゜ベンド内層流の凝固閉そく限界 : 曲円管流の無次元整理に関連して
- 垂直平板の層流自然対流による冷却 : 空気中,非金属平板の場合
- 流体と固体の伝熱が連成する熱伝達について : 方向性次元解析の立場からする一般的検討