短繊維強化ポリエーテルエーテルケトンの引張疲労特性に及ぼす平均応力の影響(<特集>疲労)
スポンサーリンク
概要
- 論文の詳細を見る
In order to characterize the fatigue strength of injection moulding advanced thermopastic, such as Polyetheretherketon(PEEK), short glass fiber reinforced PEEK(GF/PEEK)and short carbon fiber reinforced PEEK(CF/PEEK), the fatigue tests were conducted under tension-tension cylic loading(stress ratio, R=0.1〜0.7)at23±1°C, 50±5% RH. The effects of repeated stress amplitude, mean stress, characteristic of matrix and the kind of reinforced short fibers on the fatigue strength were investigated on the basis of the fractographic examination of fatigue fracture surface. The results are summarized as follows.(1)The influence of repeated stress amplitude and mean stress on the fatigue characteristic of PEEK series were revealed.(2)It was found that the effect of short fiber reinforcement on the fatigue strength characteristic is not high, the same as that on the static strength of PEEK series.(3)The short fiber reinforcement of those materials was also discussed on the basis of fractographic examination.
- 社団法人日本材料学会の論文
- 1997-10-15
著者
関連論文
- (4)一方向カーボン/エポキシ積層板のモードI層間破壊特性
- 一方向カーボン/エポキシ積層板のモードI層間破壊特性
- CFRPの面内破壊じん性 : 第1報,試験方法の検討
- カーボンクロス強化複合材料の破壊じん性とAE
- 328 CFRP複合材料の破壊とAE(複合材料)
- 含浸不良のFRPの非破壊検査法(強化プラスチックス小特集)
- 欠陥のある繊維強化プラスチックスのアコースティック・エミッション
- 織物状補強材を用いた複合材料の破壊挙動 : I. 内部応力分布と静的挙動
- 短繊維強化熱可塑性プラスチックの引張り疲労特性に及ぼす繰返し速度の影響
- 短繊維強化ポリエーテルエーテルケトンの引張疲労特性に及ぼす平均応力の影響(疲労)
- 短繊維強化ポリエーテルサルホンの引張疲労特性に及ぼす平均応力の影響(疲労)
- CFRPおよびCF/GF三層FRPの曲げクリープ特性に関する時間-温度換算則の適用性
- 熱可塑性プラスチックの疲労特性に及ぼす強化繊維および配向性の影響
- FRP三層ハイブリッド板のクリープ特性(強化プラスチックス小特集)
- 硬質プラスチックの平面曲げ疲労特性 : 設計データとしての総合
- 硬質プラスチックの疲労強度に及ぼす試験条件の影響
- 赤外線サーモグラフィによるCFRP複合材料の欠陥検出
- 炭化ケイ素連続繊維強化金属SiC_/6061Alの疲労き裂進展特性の評価
- 立方体集合組織を有する銅板を疲労き裂伝ぱの異方性
- 炭素繊維強化ポリアミドのステップ昇温によるクリープ特性の評価(高分子系複合材料)
- 230 FRP の低サイクル疲労試験時の AE 現象
- 2-12 正常および変性海綿骨の力学特性と内部構造との関係について
- 耐久性(クリープ,応力緩和,疲労,摩耗)