熱間圧延における高圧水脱スケール時の鋼材の温度低下
スポンサーリンク
概要
- 論文の詳細を見る
When scale formed during reheating and continuous rolling of steel strips is commonly by hydraulic descaling, a temperature drop of the strips inevitably occurs. On an experimental survey of parameters which had been expected to control the descaling behaviours, the temperature drop of steel strips on removing the secondary scale by hydraulic descaling was measured precisely on the basis of design of experiments. It was found that the temperature drop has correlations with the water consumption V at a pressure of 9.8MPa, interaction between V and the distance H between the steel and the nozzle, water pressure P. The temperature drop ΔT_D(℃) of steel strips by hydraulic descaling can be then expressed by the descaling parameters as follows ; ΔT_D=451.7PV/H^2+9.54 It is concluded that H should be increased with V to keep the temperature drop small when a certain pressure impact pressure is required to remove the secondary scale.
- 社団法人日本鉄鋼協会の論文
- 1991-09-01
著者
-
和田 忠義
新日本製鉄堺製鉄所
-
押見 正一
新日本製鉄(株)鉄鋼研究所
-
上田 正雄
新日本製鉄(株)堺技術研究部
-
上田 正雄
新日本製鉄(株)堺技術研究部:(現)ホタニ商事(株)
-
和田 忠義
新日本製鉄(株)鉄鋼研究所:(現)新日本製鉄(株)人事部
関連論文
- 425 連鋳機ピンチロールの損耗調査(ロール・圧延潤滑, 加工, 日本鉄鋼協会 第 102 回(秋季)講演大会)
- 736 熱延鋼板の二次スケール密着性に及ぼす巻取温度の影響(薄鋼板 (2), (3), 材料, 日本鉄鋼協会第 106 回(秋季)講演大会講演)
- 104 溶鋼注入時の湯面上昇について(造塊, 製鋼, 日本鉄鋼協会 第 97 回(春季)講演大会)
- 熱間圧延における高圧水脱スケール時の鋼材の温度低下
- 熱間圧延における高圧水脱スケール時の衝突圧
- ほうろう層の泡発生機構
- 147 10%Ni-Mo-Cr-Co-C 鋼の析出強化におよぼす合金元素の影響(熱処理・組織, 加工・性質, 日本鉄鋼協会 第 83 回(春季)講演大会)
- 鋼塊の表面欠陥に及ぼす鋳型塗料の影響
- 192 鋼塊表面疵に及ぼす鋳型塗料の影響(鋼塊品質, 製鋼, 日本鉄鋼協会 第 105 回(春季)講演大会)