熱間圧延における高圧水脱スケール時の衝突圧
スポンサーリンク
概要
- 論文の詳細を見る
Hydraulic descaling is commonly used to remove scale formed during reheating and continuous rolling of steel strips. On an experimental survey of parameters which affect the descaling behaviour, impact pressure was measured precisely both by spraying over a plasticine (a modelling material) on the basis of design of experiments and by using a pressure converter. It was found that the impact pressure has good correlations with the water consumption V at a pressure of 9.8MPa, water pressure P, rolling speed ν and distance H between the material and the nozzle. The thickness loss Δt of plasticine and the impact pressure p by hydraulic descaling can be then expressed by the descaling parameters as follows ; Δt=2000PV/(νH^2) (cm, correlation coefficient : 0.94) p=5.64PV/H^2(MPa) The impact pressure calculated from the equation is in excellent agreement with H. HOJAS' results. Since the impact pressure required to remove the primary scale is much higher than secondary scale, a careful set up of the conditions is essential to complete the descaling.
- 社団法人日本鉄鋼協会の論文
- 1991-09-01
著者
-
和田 忠義
新日本製鉄堺製鉄所
-
押見 正一
新日本製鉄(株)鉄鋼研究所
-
上田 正雄
新日本製鉄(株)堺技術研究部
-
上田 正雄
新日本製鉄(株)堺技術研究部:(現)ホタニ商事(株)
-
和田 忠義
新日本製鉄(株)鉄鋼研究所:(現)新日本製鉄(株)人事部
関連論文
- 425 連鋳機ピンチロールの損耗調査(ロール・圧延潤滑, 加工, 日本鉄鋼協会 第 102 回(秋季)講演大会)
- 736 熱延鋼板の二次スケール密着性に及ぼす巻取温度の影響(薄鋼板 (2), (3), 材料, 日本鉄鋼協会第 106 回(秋季)講演大会講演)
- 104 溶鋼注入時の湯面上昇について(造塊, 製鋼, 日本鉄鋼協会 第 97 回(春季)講演大会)
- 熱間圧延における高圧水脱スケール時の鋼材の温度低下
- 熱間圧延における高圧水脱スケール時の衝突圧
- ほうろう層の泡発生機構
- 147 10%Ni-Mo-Cr-Co-C 鋼の析出強化におよぼす合金元素の影響(熱処理・組織, 加工・性質, 日本鉄鋼協会 第 83 回(春季)講演大会)
- 鋼塊の表面欠陥に及ぼす鋳型塗料の影響
- 192 鋼塊表面疵に及ぼす鋳型塗料の影響(鋼塊品質, 製鋼, 日本鉄鋼協会 第 105 回(春季)講演大会)