鋼塊の表面欠陥に及ぼす鋳型塗料の影響
スポンサーリンク
概要
- 論文の詳細を見る
This work was carried out to obtain the information on the function of mould coatings most necessary to reduce surface defects in ingots. Thermobalance and differential thermal analyses and small scale casting experiments were carried out so that splash boxes and splash like scabs could be related to the thermal decomposition temperature of mould coatings. It is concluded that water soluble resin coatings cause so called rolling reaction of hot metal at the first stage of pouring and promote a smooth hot metal rise in the moulds and ingot surfaces appear to be the best. Coal tar and graphite of low and high thermal decomposition temperature are the causes of many surface defects in ingots.
- 社団法人日本鉄鋼協会の論文
- 1987-04-01
著者
関連論文
- 294 ヘリウムガスキャリアー・溶融熱伝導度測定法による鋼中微量窒素の迅速定量法について(分析, 加工・性質, 日本鉄鋼協会 第 78 回(秋季)講演大会)
- 736 熱延鋼板の二次スケール密着性に及ぼす巻取温度の影響(薄鋼板 (2), (3), 材料, 日本鉄鋼協会第 106 回(秋季)講演大会講演)
- 104 溶鋼注入時の湯面上昇について(造塊, 製鋼, 日本鉄鋼協会 第 97 回(春季)講演大会)
- 熱間圧延における高圧水脱スケール時の鋼材の温度低下
- 熱間圧延における高圧水脱スケール時の衝突圧
- ほうろう層の泡発生機構
- 鋼塊の表面欠陥に及ぼす鋳型塗料の影響
- 192 鋼塊表面疵に及ぼす鋳型塗料の影響(鋼塊品質, 製鋼, 日本鉄鋼協会 第 105 回(春季)講演大会)