Dependence of notch strength ratio on stress triaxiality and strain hardening exponent was investigated for a variety of structural steels. Both the notched specimens with different notch acuities and the unnotched specimens were employed to obtain a wide range of stress triaxialitity. All specimens were loaded up to break under tensile loading. Notch strength ratio was defined by a ratio of notch tensile strength to tensile strength of the material. The notch tensile strength to break the notched specimen depends on the stress-state characterized by stress triaxiality. Notch strength ratio increased with increasing stress triaxiality, which eventually reached the limiting value in the range of high stress triaxiality. The limiting notch strength ratio was well correlated with strain hardening exponent, and could be used conveniently to estimate the upper limit load to break the mechanical component in failure analysis.
- 一般社団法人日本機械学会の論文
- 2008-09-16
著者
関連論文
- G0301-6-1 切欠引張強さ比と限界ひずみ比の関係(材料力学部門一般(6))
- 1253 構造用鋼材における切欠引張強さ比の応力三軸度依存性(G03-9 材料力学(9)疲労・強度2,21世紀地球環境革命の機械工学:人・マイクロナノ・エネルギー・環境)
- 2126 応力三軸度の変化に伴う切欠試験片の最大引張強さの変化特性(G03-4 材料特性,G03 材料力学)
- 435 切欠試験片の最大応力と引張強さの比率の変化特性(変形と計測,一般セッション)
- 656 球状黒鉛鋳鉄のマクロ破断面の変化特性(機械材料・材料加工,人体のコンピュータモデルの作成とその応用,特別講演)
- 1305 最大ディプルサイズの分布と破壊挙動との関係(G03-1 き裂進展・破面解析,G03 材料力学)
- フェライト基地球状黒鉛鋳鉄のディンプル破断面の統計的評価(G03-2 き裂・破壊,G03 材料力学)
- 1031 最大ディプルサイズの分布特性と破壊挙動との関係
- 620 構造用鋼材におけるディンプル破断面の統計的評価
- GS0802 構造用鋼材における切欠引張強さ比の応力三軸度およびひずみ硬化指数依存性(GS08-01 構造部材・強度評価1,GS08 構造部材・強度評価)