Dependence of maximum tensile strength of notched specimen on stress triaxiality was investigated for a variety of structural steels. Both the notched specimens with different notch acuity and the unnotched specimens were employed to obtain a wide range of stress triaxiality. All specimens were loaded to break under tensile loading at room temperature. A marked increase in the maximum tensile strength to break the notched specimen was observed with increase in stress triaxiality. Similarly, a ratio of the maximum tensile strength to tensile strength increased with increasing stress triaxiality, which eventually reached the upper limit ratio in the range of high stress triaxialities. It is expected that those limiting ratios ranging from 1.7 to 1.95 for various materials could be used to estimate the maximum loads applied to the mechanical components.
- 一般社団法人日本機械学会の論文
- 2007-09-07
著者
関連論文
- G0301-6-1 切欠引張強さ比と限界ひずみ比の関係(材料力学部門一般(6))
- 1253 構造用鋼材における切欠引張強さ比の応力三軸度依存性(G03-9 材料力学(9)疲労・強度2,21世紀地球環境革命の機械工学:人・マイクロナノ・エネルギー・環境)
- 2126 応力三軸度の変化に伴う切欠試験片の最大引張強さの変化特性(G03-4 材料特性,G03 材料力学)
- 435 切欠試験片の最大応力と引張強さの比率の変化特性(変形と計測,一般セッション)
- 656 球状黒鉛鋳鉄のマクロ破断面の変化特性(機械材料・材料加工,人体のコンピュータモデルの作成とその応用,特別講演)
- 1305 最大ディプルサイズの分布と破壊挙動との関係(G03-1 き裂進展・破面解析,G03 材料力学)
- フェライト基地球状黒鉛鋳鉄のディンプル破断面の統計的評価(G03-2 き裂・破壊,G03 材料力学)
- 1031 最大ディプルサイズの分布特性と破壊挙動との関係
- 620 構造用鋼材におけるディンプル破断面の統計的評価
- GS0802 構造用鋼材における切欠引張強さ比の応力三軸度およびひずみ硬化指数依存性(GS08-01 構造部材・強度評価1,GS08 構造部材・強度評価)