Cavitation erosion resistance was studied for duplex stainless steels (DP33, DP37 and DP38) and super duplex stainless steels (DP40 and DP42) using a vibratory apparatus in distilled water and seawater. In comparison with the effect of the difference of the component element content on cavitation erosion resistance, following facts were clarified. Cavitation erosion resistance of the duplex stainless steels and the super duplex stainless steels in the distilled water and P.I. value which showed the corrosion-resistance did not show the good correlation. Cavitation erosion resistance in distilled water and seawater showed the good correlation with Vickers microhardness (HV) which was obtained from the ratio of ferrite phase to austenite phase and each hardness by a composite rule, and the cavitation erosion resistance are improved when the hardness increases.
- 一般社団法人日本機械学会の論文
- 2008-04-25
著者
-
望月 敬美
東京海洋大学海洋科学部神鷹丸III
-
服部 修次
福井大学大学院工学研究科
-
横田 源弘
水産大学校海洋機械工学科
-
杉山 憲一
(株)荏原総合研究所 材料研究室
-
横田 源弘
水産大学校
-
杉山 憲一
荏原総合研究所
-
岸本 守央
福井大学大学院工学研究科
-
服部 修次
福井大・工
-
横田 源弘
水産大学校機関学科
関連論文
- 二段環境下のキャビテーション壊食
- 鉄鋼材料の長時間のキャビテーション壊食
- 加速度計を用いた噴流法キャビテーション初生の検出とオリフィスキャビテーションへの応用(流体工学,流体機械)
- 523 Ti-Ni形状記憶合金肉盛材の耐キャビテーション壊食性(非鉄金属の疲労強度,一般セッション)
- キャビテーション壊食とスラリー摩耗の複合損傷に及ぼす材料特性の影響
- 903 キャビテーション壊食とスラリー摩耗機構の比較
- 1204 キャビテーション壊食とスラリ摩耗の複合損傷
- 905 ステライト合金のキャビテーション壊食とスラリー摩耗の複合損傷(O.S.8-4 強度と環境)(オーガナイズドセッション8 : 材料強度のミクロとマクロ)
- 衝撃力センサーと加速度センサーを用いたキャビテーション壊食初生評価
- 眼鏡フレームのデザイン・製造(デザイン×技術=ものづくり)