たばこ刻みの微細構造と吸着水の存在形態
スポンサーリンク
概要
- 論文の詳細を見る
The pore-size distribution and the state of water adsorbed on tobacco cut-fillers were examined by a nitrogen adsorption method and differential scanning calorimetry. The pore-size was distributed in the region of 1 to 5 nm in radius, and the population was the maximum at approximately 2 nm in radius. The results of differential scanning calorimetry showed that the amounts of nonfreezing water in Bright and Burley tobacco were 0.24 and 0.20 [kg of adsorbed water/kg of dry tobacco], respectively. These values well agreed with the amounts of water at adsorption equilibria at p/p°=0.8. The calculated thickness of the adsorbed water layer was 0.55 nm corresponding to that of 2 molecular layers, and most of the micro-pores in tobacco cut-fillers were considered to be filled with water at p/p°=0.8. Freezing water is surmised to be that of multi-layer adsorption.
- 社団法人日本農芸化学会の論文
- 1995-10-01
著者
-
中西 幸雄
日本たばこ産業株式会社たばこ中央研究所
-
中西 幸雄
日本たばこ産業(株)たばこ中央研究所
-
坂本 幸司
日本たばこ産業(株)たばこ中央研究所
-
中西 幸雄
日本たばこ産業 たばこ中研
-
中西 幸雄
日本たばこ産業 (株) たばこ中央研究所
関連論文
- シガレット包装用紙材料の機能評価法の開発
- 香りを楽しむ -たばこの香り-
- 葉タバコへの揮発性保湿剤 - 水蒸気系の2成分吸着平衡
- たばこ刻み集合体の圧縮特性における吸着水の影響
- たばこ刻みの微細構造と吸着水の存在形態
- たばこ刻みの細孔分布測定のための脱水条件の検討
- 連続V型混合機のホールドアップ特性と混合特性
- たばこ刻みの細孔分布測定のための脱水条件の検討
- 薄層植物材料へのエタノールの拡散
- 収縮性植物材料への水とエタノール混合蒸気の吸着平衡
- 薄層材料への香料滴の浸透
- 収縮性植物材料の細孔分布測定について