常圧焼結窒化けい素の常温におけるねじり疲労強度
スポンサーリンク
概要
- 論文の詳細を見る
For strength design of ceramic parts, static, static fatigue and cyclic fatigue torsional tests were carried out at room temperature on smooth specimens and notched specimens of sintered Si_3N_4. (1) The cyclic fatigue strength (maximum principal stress) at stress ratio R=0 was lower than the static fatigue strength. This was due to the effect of cyclic stress. The cyclic fatigue strength at stress ratio R=-1 was lower than that at R=0. This difference was almost equal to the difference in strength calculated from the effective volume. In this case, the effective volume of R=-1 is twice as much as that of R=0. (2) In the case of a gentle notch, both static torsional strength and cyclic torsional strength increased unlike in the case of static plane bending and rotating bending respectively. This can be accounted for by the difference in the effective volume.
- 社団法人日本機械学会の論文
- 1989-07-25
著者
関連論文
- ダイカスト用金型鋼の疲労亀裂進展特性
- 塑性締めボルトの疲労強度 : 再使用時の疲労強度保証
- 131 塑性締めボルトの疲労強度 : 再使用時の疲労強度保証(疲労強度II)
- 熱間金型鋼SKD62の疲労き裂進展特性に及ぼす焼入冷却速度の影響
- 101 焼入冷却速度による熱間型鋼SKD62の疲労き裂進展特性の変化(疲労き裂進展)
- 109 熱間金型鋼SKD62の疲労き裂進展特性に及ぼす高温焼入れの影響(疲労き裂進展に対する影響因子)
- 共振を利用した歯車疲労試験機の開発
- タフトライド処理を施した球状黒鉛鋳鉄および片状黒鉛鋳鉄の耐久限度線図
- 熱間加工を施したTiB粒子強化型Ti基MMCの組織と機械的性質
- 窒化けい素セラミックスの微細構造と疲労特性の関係(疲労)