オーステンパ球状黒鉛鋳鉄の二段折れ曲り破壊機構
スポンサーリンク
概要
- 論文の詳細を見る
Very high cycle fatigue tests were conducted on austempered ductile iron finished by buffing (called material A) and that finished by electropolishing (called material EA) for comparison of what please clarity. An S-N curve of rotating bending fatigue of material A represented a characteristic of a two-stage bending resembling extremely high-strength materials. This phenomenon clarified the occurrence of different fracture mechanisms through the intermediary of nonpropagating cracks. In material EA, the structural sensitivity was lower owing to the removal of the work hardening layer on the material surface. Consequently, its S-N curve of rotating bending fatigue was unexceptional, because mechanical properties of its matrix structure resemble those of its pearlitic structure. Fatigue stress amplitudes of both materials were σ_w = 382 MPa.
- 一般社団法人日本機械学会の論文
- 1995-11-25
著者
関連論文
- キーみぞ軸の寸法効果
- シャフトのねじり疲れ強さ
- 723 表面改質球状黒鉛鋳鉄の疲労強度信頼性評価
- 637 イオン浸炭処理切欠き PDI 材の疲労強度特性
- DLCと種々のTi系薄膜のフラクタル特性(GS8 マイクロ/ナノ試験・薄膜)
- 117 薄膜打痕表面のレーザー顕微鏡観察とフラクタル次元解析(薄膜,疲労の機構と強度信頼性,オーガナイスドセッション1,第53期学術講演会)
- K-0532 軽荷重打撃による表面薄膜のフラクタル解析(S04-5 小型・薄板材の疲労と実機信頼性)(S04 金属材料の組織と疲労強度信頼性)
- 球状黒鉛鋳鉄の疲労挙動 : 第2報,高サイクル疲労に及ぼす微小欠陥の影響
- 球状黒鉛鋳鉄の高サイクル疲労挙動 : 第1報,オーステンパ処理材の疲労強度に及ぼす試験片寸法および採取位置の影響
- ガス浸炭炉熱処理を施したPDI材とADI材の高サイクル疲労強度および耐摩耗性の比較評価
- 708 焼結合金WC-Coの破壊じん性評価(変形・強度,一般セッション)
- 薄膜打痕表面のレーザー顕微鏡観察とフラクタル次元解析(GS8 マイクロ/ナノ試験・薄膜)
- 362 軽荷重打撃による表面薄膜のフラクタル解析(OS1-6 熱影響部と配管の健全性評価)(OS1 高強度材・表面改質材の疲労と破壊)
- 熱環境下におけるオーステンパ球状黒鉛鋳鉄の疲労強度
- WWWブラウザと分散オブジェクトを用いた有限要素解析システムの構築
- 雰囲気温度におけるオーステンパ球状黒鉛鋳鉄の高サイクル疲労挙動
- オーステンパ球状黒鉛鋳鉄の長寿命域における回転曲げ疲労
- オーステンパ球状黒鉛鋳鉄の二段折れ曲り破壊機構
- オーステンパ球状黒鉛鋳鉄の疲労強度に及ぼす油環境の影響
- オーステンパ球状黒鉛鋳鉄の高サイクル疲労特性 : 電解研磨による表面加工層除去の影響
- オーステンパ球状黒鉛鋳鉄の長寿命域における疲労挙動
- 球状黒鉛鋳鉄の疲労破面解析と黒鉛の挙動
- 炭素鋼の疲れと残留応力(回転曲げ)
- オーステンパ球状黒鉛鋳鉄の高サイクル疲労に及ぼす表面硬さの影響