球状黒鉛鋳鉄のねじり疲労強度に及ぼす人工微小欠陥と黒鉛の影響(<特集>疲労)
スポンサーリンク
概要
- 論文の詳細を見る
Reversed torsion and rotating bending fatigue tests were performed on JIS FCD400 using both smooth and defect specimens containing an artificial hole whose diameter ranges from 100 to 500 μm. Although this material has numerous spheroidal graphites in the structure, the effect of interaction between defects on the fatigue limit was so small that the fatigue limit of specimen containing an artificial hole was predicted from √<area> for the hole and the Vickers hardness of matrix by the equation that was proposed in this study assuming steels with a single defect. The fatigue limit of smooth specimens in torsion was controlled by graphites and the lower bound of the scatter was well predicted substituting the size of the maximum graphite, √<area>_<max> for √<area> in the equation. The value of √<area>_<max> may correspond to the allowable defect size of this material.
- 社団法人日本材料学会の論文
- 1996-01-15
著者
関連論文
- S45C焼なまし材のねじり疲労に及ぼす人工微小欠陥の影響 : 曲げとの比較
- 軸受鋼SUJ2における微小疲労き裂のせん断型進展と下限界
- 極めて浅い切欠きをもつ炭素鋼の疲労強度 : 連続観察をもとにした考察
- 10-104 機械工学における基礎製図の現状と課題((2)専門科目の講義・演習-I)
- 2-325 3Dアニメーションを駆使した設計製図学習用ソフトウェアの開発((11)教育ソフトウエア-II)
- 組合せ荷重下にある微小穴材の疲労強度に及ぼす位相差と平均応力の影響の予測
- 応力集中部から進展するき裂の塑性域寸法の解析
- Art McEvily 80歳誕生日記念シンポジウム : Fatigue and Fracture of Traditional and Advanced Materialsに参加して
- 球状黒鉛鋳鉄のねじり疲労強度に及ぼす人工微小欠陥と黒鉛の影響(疲労)
- 最近の球状黒鉛鋳鉄の疲労強度に及ぼす黒鉛と人工微小欠陥の影響(破壊力学特集)
- A17 組合せ応力疲労下の微小モードIき裂の進展と下限界(OS5 材料の変形・破壊の計測・解析と損傷評価IV)
- 切欠き材の疲労き裂発生寿命と破断寿命の予測
- 時効硬化Al合金の回転曲げ疲労における切欠き感度 : 微小切欠き材による検討
- 焼もどし温度をかえたS45C焼入れ焼もどし材の疲労過程の相違
- 疲労強度に及ぼす微小欠陥の影響の評価法
- 高硬さ鋼の疲労過程
- 組合せ応力をうける球状黒鉛鋳鉄の疲労強度評価
- 球状黒鉛鋳鉄の疲労強度に及ぼす黒鉛の形状, 寸法, 分布の影響
- 微小き裂の下限界応力拡大係数幅ΔK_ に及ぼす硬さとき裂形状の影響
- 疲労における切欠き効果の統一的取扱い