連続焼鈍缶用鋼板の耐フルーティング性を支配する冶金的因子
スポンサーリンク
概要
- 論文の詳細を見る
Effects of annealing temperature and primary cooling rate in continuous annealing on the fluting resistance of soft temper tinplate were experimentally investigated. Based on its result, the influence of grain size, solute carbon and carbide morphology affecting the fluting resistance was studied. Main results are the following : The more rapid the cooling rate is and the higher the annealing temperature is, the better the fluting resistance is improved. However, the dependency of the fluting resistance on cooling rate becomes small with the annealing temperature. Therefore, high temperature annealing is most effective and rapid cooling is second most effective to keep the fluting resistance acceptable under the normal reduction rate of temper rolling. These results mean that coarsening of grains is most effective, and the reduction of solute carbon is second most effective especially in the case of insufficient grain coarsening. Materials with fine and dispersed morphology of carbide show better fluting resistance than those with aggregated carbide on grain boundaries even if the grain size and solute carbon content are the same with each other.
- 社団法人日本鉄鋼協会の論文
- 1996-06-01
著者
関連論文
- 337 連続焼鈍によるブリキ原板のテンパー度制御技術 : 薄手用連続焼鈍技術の開発第 2 報(冷延薄板, 焼鈍炉, 加工・システム, 日本鉄鋼協会第 108 回(秋季)講演大会)
- 647 冷延鋼板の材質に及ぼすスキンパス歪速度の影響(複合組織鋼板・薄板, 材料, 日本鉄鋼協会 第 105 回(春季)講演大会)
- 高圧下調質圧延による軟質缶用鋼板の耐フルーティング性の改善
- 焼付硬化性鋼板の 2 ピース缶軽量化への適用
- 連続焼鈍缶用鋼板の熱延板固溶 N 量に及ぼす Al 量の効果
- 連続焼鈍冷延鋼板の高張力化におよぼす合金元素と焼鈍サイクルの影響 : 一般加工用高強度自動車用冷延鋼板の開発(冷延鋼板)(高強度薄鋼板)
- 744 冷延鋼板の調質圧延による変形帯と残留歪分布(薄鋼板 (2), (3), 材料, 日本鉄鋼協会第 106 回(秋季)講演大会講演)
- 675 軟質ぶりき原板の耐フルーティング性におよぼす高速冷却の効果 : 薄手用連続焼鈍技術の開発 5(薄鋼板 (III), 材料, 日本鉄鋼協会第 114 回(秋季)講演大会)
- 連続焼鈍で製造される缶用鋼板の軟質化に及ぼす N の影響
- 409 連続焼鈍軟質ぶりき原板の耐フルーティング性におよぼす高圧下スキンパスの効果 : 薄手用連続焼鈍技術の開発 4(缶用鋼板, 討論会, 分析・表面処理, 日本鉄鋼協会第 113 回(春季)講演大会)
- 連続焼鈍缶用鋼板の耐フルーティング性を支配する冶金的因子