JIS R 1607三点曲げ破壊靭性試験片のコンプライアンスと応力拡大係数の解析
スポンサーリンク
概要
- 論文の詳細を見る
To use for single specimen determination of R-curve with three-point bending of JIS R 1607 type II specimen (span-to-width ratio, S/W=7.5), calculation formulas for analyses with the elastic compliance method are presented. Numerical analyses of stress intensity factor and specimen compliance are carried out and based on these results, crack length and stress intensity factor are expressed as functions of specimen compliance. These are defined in the entire range of crack length relative to specimen width, a/W. A formula of a/W as a function of specimen compliance, inverse compliance, is also derived. In this procedure, two different techniques, boundary collocation and finite element method, are performed independently. The results of the both calculation show good agreement in the most range of a/W and the uncertainty is estimated to be within 0.8%. The reliability of proposed formulas is also examined in experiments. Crack length and stress intensity factor of borosilicated glass samples are calculated with proposed formulas and verified with other experimental facts. As a result of these experiments the reliability of calculated values is estimated to be within 3%.
- 公益社団法人精密工学会の論文
- 2002-06-05
著者
関連論文
- 振動加速度計の校正における外乱要因とその補正
- 振動加速度計の校正における電荷増幅器の影響
- 振動加速度標準における電荷増幅器の校正法
- P3-40 位相共役光干渉計を用いた表面き裂の画像化に関する研究(ポスターセッション3(概要講演))
- レーザー超音波による精密音速測定と半導体プロセスの温度計測への応用
- 電子顕微鏡内超微小押込み試験機の開発
- 変位計測による押し込み変位同時計測
- ナノインデンテーションの有限要素解析による圧子先端形状の影響に関する検討
- 光干渉計を備えた小型ナノインデンテーション装置の試作
- 光ファイバ干渉計を備えた小型ナノインデンテーション装置の試作
- 走査電子顕微鏡用ナノインデンテーション装置の開発 -(第2報) 押込み深さ測定用光ファイバ干渉計の製作-
- JIS R 1607三点曲げ破壊靭性試験片のコンプライアンスと応力拡大係数の解析
- コンプライアンス法によるセラミックス三点曲げ試験片のき裂長さと応力拡大係数の連続測定
- セラミックスの安定破壊が可能な三点曲げ試験装置の開発
- き裂長さの適用範囲を拡大したJIS R-1607破壊じん性試験片の応力拡大係数とコンプライアンスの計算式
- セラミックスの安定破壊が可能な三点曲げ試験装置の開発
- ナノインデンテーションの標準設定にむけて
- 硬さ試験と計量標準
- ナノインデンテーション用圧子先端形状の計測技術と押込み試験への影響