Blistering Behavior during Oxide Scale Formation on Steel Surface
スポンサーリンク
概要
- 論文の詳細を見る
- 2011-09-15
著者
-
近藤 泰光
新日本製鉄(株)環境・プロセス研究開発センター
-
Ushioda Kohsaku
Technical Dev. Bureau Nippon Steel Corp.
-
KONDO Yasumitsu
Steel Rolling R&D div., Environment & Process Technology Center, Technical Development Bureau, Nippon Steel Corporation
-
TANEI Hiroshi
Steel Rolling R&D div., Environment & Process Technology Center, Technical Development Bureau, Nippon Steel Corporation
-
SUZUKI Noriyuki
Steel Rolling R&D div., Environment & Process Technology Center, Technical Development Bureau, Nippon Steel Corporation
-
MAEDA Muneyuki
Oita works, Nippon Steel Corporation
-
Tanei Hiroshi
Steel Rolling R&d Div. Environment & Process Technology Center Technical Development Bureau Nippon Steel Corporation
-
Kondo Yasumitsu
Steel Rolling R&d Div. Environment & Process Technology Center Technical Development Bureau Nippon Steel Corporation
-
Kondo Yasumitsu
Environment & Process Technology Center Nippon Steel Corporation
-
Kondo Yasumitsu
Environment & Process Technology Centre Nippon Steel Corporation
-
Suzuki Noriyuki
Steel Rolling R&d Div. Environment & Process Technology Center Technical Development Bureau Nippon Steel Corporation
関連論文
- 銅含有鋼の高温酸化時におけるスケール/地鉄界面への濃化銅量に及ぼす雰囲気条件の影響-3
- Cu含有鋼の高温酸化時におけるスケール/地鉄界面への濃化Cu量に及ぼす雰囲気条件の影響-2
- Cu含有鋼の高温酸化時におけるスケール/地鉄界面への濃化Cu量に及ぼす雰囲気条件の影響
- 温度非定常条件での低炭素鋼の高温酸化挙動
- 低酸素濃度雰囲気での低炭素鋼の高温酸化
- 低炭素鋼の高温酸化に及ぼす水蒸気の影響
- Deep Drawability of Electro-deposited Pure Iron Having an Extremely Sharp //ND Texture
- The Effect of S and Mn on the High-temperature Oxidation and Scale Spallation Behavior of Low-carbon Steels
- Analysis of Flange Wrinkle in Square-shell Deep Drawing of Anisotropic Sheet
- Evolution of Dislocation Structure and Fatigue Crack Behavior in Fe-Si Alloys during Cyclic Bending Test
- Cold-rolling and Recrystallization Texture Formation in Electro-deposited Pure lron with a Sharp and Homoqeneous γ-fiber
- Comparison of the Dislocation Density in Martensitic Steels Evaluated by Some X-ray Diffraction Methods
- Role of TiAl_3 Fine Precipitate in Nucleation of the Primary Al Dendrite Phase during Solidification in Hot-Dip Zn-11%Al-3%Mg-0.2%Si Coated Steel Sheet
- Blistering Behavior during Oxide Scale Formation on Steel Surface
- The Increase in a Brittle-to-ductile Transition Temperature in Fe-Al Single Crystals
- Behaviour of Cu at High Temperature Oxidation of Cu containing steel
- Effects of Initial Scale Structure on Transformation Behavior of Wustite
- Effect of Nitrogen on Blister Growth Process during High Temperature Oxidation of Steel
- Effect of Atmospheric Conditions on Copper Behaviour during High Temperature Oxidation of a Steel Containing Copper
- Behaviour of Copper during High Temperature Oxidation of Steel Containing Copper
- Influence of Si Addition to the Coating Bath on the Growth of the Al-Fe Alloy Layer in Hot-dip Zn-Al-Mg Alloy-coated Steel Sheets
- Role of Hematite Formation on Blister Generation during High Temperature Oxidation of Steel
- 鋼表面のスケール生成時におけるブリスタリング挙動
- Effect of Carbide Size Distribution on the Impact Toughness of Tempered Martensitic Steels with Two Different Prior Austenite Grain Sizes Evaluated by Instrumented Charpy Test
- Behavior of High-Temperature Embrittlement and Its Mechaism in Heat-Affected Zone of Low-Carbon Alloy Steels