In order to improve the fracture toughness of intrinsically brittle ceramics, it is essential to expand the frontal process zone (FPZ) ahead of a crack tip. Nanocomposites proposed by Niihara utilize dislocations generated around the dispersed nano-sized particles in matrix and expand the FPZ. In this paper, we discussed the toughening mechanism of ceramics using our experimental data on alumina-based nanocomposites, focusing on fundamental theories of fracture mechanics, such as Griffith-Irwin energy equilibrium and the local fracture criterion. We estimated the FPZ size using an indirect technique proposed recently, and clarified that the FPZ expansion toughening mechanism is achieved in nanocomposites by means of dislocation activities. The results revealed that ceramics with a larger FPZ size had higher fracture toughness and properly annealed nanocomposites had the largest FPZ size. The FPZ expansion mechanism in nanocomposites was considered that sessile dislocations generated around a crack tip in matrix, served as nano-crack nuclei, and hence expanded the FPZ size. It is clarified that the critical local stress is the strength of an infinite plate with no crack, and must be the true strength with no size effect. The fracture toughness, the critical local stress, and the FPZ size are the mutually dependent material properties, and the relation among them is clarified.
- 公益社団法人 日本セラミックス協会の論文
- 2009-05-01
著者
-
Awaji Hideo
Korea Fine Ceramics Center Gangneung Sci. Park
-
NISHIMURA Yoshitaka
Fuji Electric Device Tech., Co., Ltd.
-
CHOI Seong-Min
Fuji Electric Device Tech., Co., Ltd.
-
TAKAHASHI Yoshikazu
Fuji Electric Device Tech., Co., Ltd.
-
GOTO Tomoaki
Fuji Electric Device Tech., Co., Ltd.
-
HASHIMOTO Shinobu
Nagoya Institute of Technology
-
Choi Seong-min
Fuji Electric Device Tech. Co. Ltd.
-
Goto Tomoaki
Fuji Electric Device Tech. Co. Ltd.
-
Goto Tomoaki
Fuji Electric Advanced Technology Co. Ltd Production Technology Laboratory
-
Takahashi Yoshikazu
Fuji Electric Device Tech. Co. Ltd.
-
Hashimoto Shinobu
Department Of Environmental Materials And Engineering Nagoya Institute Of Technology
関連論文
- Toughening mechanism and frontal process zone size of ceramics
- Sintering and Mechanical Properties of Complex Carbides in the Al-Si-C System
- Strength and Thermal Shock Properties of Scandia-Doped Zirconia for Thin Electrolyte Sheet of Solid Oxide Fuel Cell
- Syntheses and crystal structures of Si-bearing layered carbides ZrAl_8C_7 and ZrAl_4C_4
- Syntheses and crystal structures of Ge-bearing layered carbides Zr_2Al_4C_5 and Zr_3Al_4C_6
- Detoxification of industrial asbestos waste by low-temperature heating in a vacuum( Innovative Ceramic Materials and Technologies for Global Environmental Protection)
- 3次元配線アレイの開発
- Relation between functional properties of alumina-based nanocomposites and locations of dispersed particles
- Synthesis and mechanical properties of Al_8B_4C_7
- キャスタブルのマトリックスにおける金属アルミニウム粉の水和に及ぼすマグネシアとアルミン酸カルシウムセメントの影響
- Interfacial Microstructure and Joint Properties of Copper Direct Bond Inserted by the Thin Film of Indium
- Mechanism for the formation of SiC by carbothermal reduction reaction using a microwave heating technique
- Effects and Behavior of Al_8B_4C_7 Added to MgO-C Refractories
- The Effect of TiO_2 Additions on the Properties of a Cr_2O_3-ZrO_2 Composite
- Effect of Added CrB_2 in MgO-C Refractories
- Microstructural Analysis of MgO-C Refractories
- Comparison of Additives in MgO-C Refractories
- Preparation and Characterization of a Porous Ceramic Sheet Composed of (Cr, Al)_2O_3 Platelet Crystals
- Mechanical Properties of Al_8B_4C_7 with Alumina Platelets
- Mechanical Properties of Al_8B_4C_7 with Alumina Platelets