In order to achieve a low number of polishing defects and to decrease surface roughness on the silicon wafers in chemical mechanical polishing (CMP) technology, the fumed silica slurry settlement method is proposed. Large particles including in the CMP slurry are known to have effects on the polishing defect and the surface roughness on the polished wafer. To stabilize the CMP slurry, the large particles are removed with the settlement separation method, which is a simple method compared to filtration or centrifuge methods. The fumed silica slurry settlement system can selectively remove the large particles which cause scratch defects during CMP. The large particles over 1.0 μm size can be selectively removed after 7 days of sedimentation. The settlement-treated slurry shows good results in terms of the defect levels and surface roughness with the plasma-tetra-ethoxy-silane (p-TEOS) oxide wafer.
- 2003-02-15
著者
-
Koubuchi Yasushi
Rodel-nitta Company
-
Fukuda Keiji
Rodel-nitta Company
-
Haba Shinichi
Department Of Electronic And Photonic Systems Engineering Kochi University Of Technology
-
Ohta Yoshiharu
Rodel-nitta Company
-
Katouda Takashi
Department Of Electronic And Photonic Systems Engineering Kochi University Technology
-
Haba Shinichi
Department of Electronic and Photonic Systems Engineering, Kochi University of Technology, Tosayamada-cho, Kami-gun, Kochi, Japan
関連論文
- 筋電位と肢体の三次元挙動を指標としたレバー式車椅子の操作性の分析
- 469 10Cr-2Mo-V-Nb 耐熱鋼における溶解法と微量添加元素の影響(耐熱鋼・耐熱合金, 性質, 日本鉄鋼協会第 101 回(春季)講演大会)
- 501 10Cr-2Mo 系耐熱鋼のクリープ破断強度と常温付近の衝撃特性(耐熱鋼・耐熱合金, 性質, 日本鉄鋼協会 第 100 回(秋季)講演大会)
- 高 Cr フェライト系耐熱鋼の加熱脆化因子
- Fumed Silica Slurry Stabilizing Methods for Chemical Mechanical Polishing
- Fumed Silica Slurry Stabilizing Methods for Chemical Mechanical Polishing
- The Effects of Nodular Colloidal Silica on Chemical Mechanical Polishing