BNCT 用リチウムターゲットにおける H2O 添加による低温・低圧窒化リチウム合成
スポンサーリンク
概要
- 論文の詳細を見る
Low temperature synthesis of lithium-nitride compound was conducted on the lithium target for BNCT by N2/H2O mixing gas squirt in the ultra high vacuum chamber, and the following results were derived; (1) Lithium-nitride compound was synthesized on the lithium target under 101.3 Pa N2 gas squirt at room temperature and in the ultra high vacuum chamber under the pressure of 1×10−8 Pa. (2)Remarkable contamination by O and C was observed on the lithium-nitride compound synthesized under the squirt pressure of 13.3~80 Pa/1.33~4.7 Pa N2/H2O mixing gas. (3) No contamination and synthesis of Li-N compound was observed under the squirt pressure of 0.013~0.027 Pa/0~0.005 Pa N2/H2O mixing gas. (4) Contamination by O and C was enhanced with excessive addition of H2O at the pressure of over 1.33 Pa.
著者
-
石山 新太郎
独立行政法人 日本原子力研究開発機構
-
藤井 亮
株式会社CICS
-
馬場 祐治
独立行政法人日本原子力研究開発機構量子ビーム応用研究部門
-
中村 勝
株式会社CICS
-
今堀 良夫
株式会社CICS
関連論文
- イオンコーティング技術による高放射線汚染土洗浄用装置の汚染防止効果
- 高放射能汚染土壌の界面化学的分散制御高速せん断流解砕洗浄による再生土化
- BNCT 用リチウムターゲットにおける H2O 添加による低温・低圧窒化リチウム合成
- ホウ素中性子捕獲療法のためのリチウムターゲット表面に合成した Li3N の表面化学状態