This study examined the effect of cyclic plastic pre-strain on low cycle fatigue life at middle high temperature to evaluate the structural integrity of the nuclear components introduced plastic strain to the local portion by the large seismic load. The materials selected in this study were austenitic steel (SUS316NG) and ferritic steel (SFVQ1A, STS410: JIS*). The low cycle fatigue tests at RT and middle high temperature (300 degrees C) were carried out using cyclic plastic pre-strained materials. The results obtained here show that the damage by the cyclic plastic pre-strain, which is equivalent to usage factor UF=0.2, does not affect the fatigue lives of the materials. In addition, it is confirmed that the estimation based on the usage factor UF can also be useful for the life prediction at 300 degrees C as well as RT.[*JIS: Japanese Industrial Standards]
著者
-
菅野 智
日立GEニュークリア・エナジー(株)
-
菅野 智
日立GEニュークリア・エナジー(株)
-
中根 一起
(株)日立製作所 日立研究所
-
髙木 愛夫
東京電力(株) 技術開発研究所
-
髙木 愛夫
東京電力(株) 技術開発研究所
関連論文
- 改良MANSON式による低サイクル疲労寿命評価法の検討(M&M2009材料力学カンファレンス)
- 低サイクル疲労寿命に及ぼす繰返し塑性予ひずみの影響(M&M2009材料力学カンファレンス)
- 低サイクル疲労寿命に及ぼす予ひずみの影響
- 改良 MANSON 式による低サイクル疲労寿命評価法の検討
- 低サイクル疲労寿命に及ぼす繰返し塑性予ひずみの影響
- 低サイクル疲労寿命に及ぼす予ひずみの影響--中越沖地震後の柏崎刈羽原子力発電所の健全性評価
- 824 ステンレス鋼および炭素鋼の疲労破面観察に関するラウンドロビン試験
- J0301-1-4 軸・捩り複合荷重下の疲労寿命評価(規格における疲労関連課題と方向性(1))
- 3216 配管系終局強度耐震実証試験 : 要素試験
- OS0746 低サイクル疲労寿命に及ぼす繰返し塑性予ひずみの影響(構造用材料の疲労挙動と寿命評価,オーガナイズドセッション)
- OS0745 改良MANSON式による低サイクル疲労寿命評価法の検討(構造用材料の疲労挙動と寿命評価,オーガナイズドセッション)
- 中高温での低サイクル疲労寿命に及ぼす繰返し予ひずみの影響
- 1701 中高温での低サイクル疲労寿命に及ぼす繰返し予ひずみの影響(OS17-1 低サイクル疲労とその応用-予ひずみ、変動荷重の影響-)