Surface irradiation damage of 316 stainless steel, vanadium and molybdenum by helium ion bombardment.
スポンサーリンク
概要
- 論文の詳細を見る
Molybdenum, V and 316 stainless steel were irradiated with 50150 keV He ions at the temperatures between 413 and 1, 298 K for total doses ranging 1 x 10<SUP>22</SUP>1 x 10<SUP>23</SUP> m<SUP>-2</SUP>, and the characteristics of the surface damage were compared. Severe exfoliation was observed in all of these materials for the irradiation at 413±110 and 748±25 K. The number of exfoliated skins was larger than that in literature, and increased nearly in proportion with the total dose. It increased in the order Mo<316SS<V. When the dose was low, the amount of erosion increased rapidly with total dose, but tended to be saturated for higher doses than 3 x 10<SUP>22</SUP> m<SUP>-2</SUP>. It increased in the order Mo<V<316 SS at 413±110 K, while in the order 316 SS<Mo<V at 748±25 K. At higher temperatures than 923 K, blisters and porous surface were formed and the exfoliation of skins ceased. The amount of erosion increased with increasing incident ion energy in the energy range between 50 and 150 keV at 413±110 K for a total dose of 1 x 10<SUP>22</SUP> m<SUP>-2</SUP>.
著者
-
Watanabe Ryoji
Natioleal Sanatatorium
-
SHIRAISHI Haruki
Tsukuba Laboratories, National Research Institute for Metals
-
SHINNO Hitoshi
Tsukuba Laboratories, National Research Institute for Metals
-
KIMOTO Takayoshi
Tsukuba Laboratories, National Research Institute for Metals
関連論文
- Studies on the Pulmonary Circuration in Patients with Pulmonary Tuberculosis (XII) : The Influence of Aging on the Pulmonary Circulation : PROCEEDINGS OF THE 25TH ANNUAL MEETING JAPANESE CIRCULATION SOCIETY (Part II)
- The Effect of Plastic Deformation on the Electrical Resistivity of a Cu-4wt% Ti Alloy with Modulated Structure
- Age-Hardening of Cu-4% Ti Alloy Due to Modulated Structure
- Deformation Twinning in Aged Cu-4% Ti Alloy
- Surface irradiation damage of 316 stainless steel, vanadium and molybdenum by helium ion bombardment.
- Precipitation in Ni-12 at. % Ti Alloy
- Corrosion behaviors of iron-base alloy, nickel-base alloy and refractory metal alloys in high-temperature impure helium gas.
- Void swelling and precipitation in Ti-modified austenitic Fe-Ni-Cr alloys.
- Void swelling of solution-annealed Type 316 stainless steel under long time proton irradiation.