重金属イオン含有排水のフェライト化処理(第2報) : Fe<SUB>3</SUB>O<SUB>4</SUB>生成に及ぼすFe(OH)<SUB>2</SUB>酸化速度の影響
スポンサーリンク
概要
- 論文の詳細を見る
The aqueous suspensions containing 0.05, 0.10 and 0.20 M Fe(II) with pH 12 were subjected to oxidation with air at 20, 40, 60 and 80°C. The time duration, θ<SUB>e</SUB>, needed for complete oxidation of Fe(II), which had been detected by the presence of dissolved oxygen in the suspension, was limited between 15 and 180 min by varing the oxidation rate.<BR>Relation between the yield of Fe<SUB>3</SUB>O, (X) and θ<SUB>e</SUB> was obtained as follows; dX/dθ<SUB>e</SUB> =k(1-X )<SUP>2</SUP> or 1/(1-X)=kθ<SUB>e</SUB>+1, where k is a function of the oxidation temperature.<BR>The Fe<SUB>3</SUB>O<SUB>4</SUB> content of the oxidation product was affected by the oxidation rate and temperature. Settling velocity of the product became faster with increasing X for X≥0.6.
- 社団法人 粉体粉末冶金協会の論文
著者
-
近藤 正樹
住友重機械工業(株)プラント・環境事業本部環境技術研究所
-
中島 信顕
住友重機械工業(株)技術本部環境技術研究所
-
平沢 輝高
住友重機械工業(株)技術本部環境技術研究所
-
近藤 正樹
住友重機械工業(株)技術本部環境技術研究所
-
中島 信顕
住友重機械工業 (株) 平塚研究所
関連論文
- Hgイオン含有排水の還元気化処理
- Zn,CdおよびMnのフェライト化処理生成物からの重金属再溶出特性
- 重金属イオン含有排水のフェライト化処理(第2報) : Fe3O4生成に及ぼすFe(OH)2酸化速度の影響
- 重金属イオン含有排水のフェライト化処理(第1報) : Fe(OH)2の空気酸化によるFe3O4生成に関する始発pHと溶存酸素について
- 超臨界炭酸ガスによるセラミックス成形体中のバインダー除去