ダイカスト金型用高信頼性熱間ダイス鋼“DHA1-ES”
スポンサーリンク
概要
- 論文の詳細を見る
Long life die casting die steels have been required to reduce die cast product cost. The main life limiting factor is premature failure. To obtain higher fracture resistance, high reliable hot work die steel, "DHA1-ES", has been developed. Generally, crack susceptibility is estimated by the Charpy impact value. It is cleared that clean and homogenized steel shows higher Charpy impact value. To improve the toughness the manufacturing process of this steel is optimized such as melting, forging and heat treatment. Though DHA1-ES has the same compositions as those of JIS SKD61, its Charpy impact values, dispersion and anisotropy are improved remarkably. Furthermore, low cycle fatigue life of this grage is longer than JIS-SKD61. It is expected that DHA1-ES is widely used in die casting industry with high reliability.
- 電気製鋼研究会の論文
著者
関連論文
- 冷間ダイス鋼の熱処理変寸の異方性に及ぼす晶出炭化物の影響
- 高濃度浸炭材の疲労強度に及ぼす炭化物析出形態の影響
- 熱処理変寸制御性に優れるマトリックス冷間ダイス鋼DCMXの開発
- ヒートチェックを克服する金型材料
- ダイカスト金型用の高熱伝導率鋼「DHA-Thermo」の開発
- 大型品対応新熱間ダイス鋼DH31-SS1の開発
- VC分散高剛性鋼の機械的性質とヤング率に及ぼす熱処理の影響 (VC分散高剛性鋼の開発-2)
- 溶製法で製造したVC分散高剛性鋼の諸特性 (VC分散高剛性鋼の開発-1)
- かち割りコンロッド用非調質鋼の開発
- 高周波焼入れ材のピッティング寿命に及ぼす有効硬化層深さとケイ素含有量の影響
- 高周波焼入材のピッティング寿命に及ぼすSi含有量の影響
- 高周波焼入材のローラーピッティング試験における最適硬化層深さ
- ベイナイト型非調質鋼の組織と機械的性質に及ぼす合金元素の影響と切欠き材の疲労強度
- 非調質鋼の切欠き引張試験破断伸びに及ぼす合金元素の影響
- V無添加フェライト+パーライト型非調質鋼の機械的性質に及ぼす合金元素の影響
- フェライト+パーライト鋼の高周波焼入後疲労強度に及ぼす初析フェライト面積率の影響
- 高強度・高靭性非調質鋼
- 非調質鋼の高応力疲労強度
- フェライト・パ-ライト型非調質鋼の機械的性質に及ぼすC,V量の影響 (構造用鋼)
- 福祉機器用低コストβ型チタン合金の疲労特性とミクロ組織
- Ti-Fe-Cr合金の相構成と引張特性に及ぼすβ単相領域温度からの冷却速度の影響
- Ti-Fe-Cr-Al合金の引張特性と時効挙動に及ぼすアルミニウム添加量の影響
- 自動車に使われる金型用鋼の最近の技術動向
- 最近の金型材料と熱処理
- 中炭素鋼の軟窒化特性に及ぼす合金元素の影響
- 熱間工具鋼の軟窒化後窒素濃度分布に及ぼす合金元素の影響
- 真空浸炭中の炭素侵入機構
- フェライト・パーライト型非調質鋼の機械的性質に及ぼすC, V量の影響
- 熱間ダイス鋼における軟窒化拡散層のTEM組織観察
- ダイカスト金型用高信頼性熱間ダイス鋼“DHA1-ES”
- 特別報告 ASEAN地域の金型事情 (特集 工具鋼)
- 丸棒鋼用自動磁粉探傷装置の開発