Al2O3-30%TiC composites doped with 0.5%MgO and 0.3-1.0% Y2O3 additives are pressureless-sintered at different conditions such as temperatures, soaking times, and heating rates under an argon atmosphere. The physical, mechanical properties, and cutting performance of sintered composites were compared with commercial one. In this work, the Al2O3-30%TiC composites doped with 0.5%MgO and 0.3%Y2O3 sintered at 1800°C obtained highest density of 97% of theoretical and flexural strength of 343 MPa. In addition, the cutting performance of the Al2O3-30%TiC-0.5%MgO-0.3%Y2O3 sintered at 1800°C was comparable with the commercial cutting tool.
- 一般社団法人 日本機械学会の論文
著者
-
ATONG Duangduen
National Metal and Materials Technology Center
-
KASURIYA Supawan
National Metal and Materials Technology Center
関連論文
- Investigation of Pyrolyzed Chars from Physic Nut Waste for the Preparation of Activated Carbon
- Effect of MgO-Y2O3 Powders and Sintering Temperature on Properties of Al2O3-TiC Composites
- A-2 EFFECT OF SINTERING TEMPERATURE AND ADDITIVES ON PROPERTIES OF Al_2O_3-TiC COMPOSITES(Session: Ceramics I)
- F-3 PREPARATION OFAl_2O_3-TiC-SiC COMPOSITES BY MICROWAVE ENERGY(Session: Composites I)
- Preparation of Al2O3-TiC Composites and Their Cutting Performance