PS53 リスク解析援用型構造健全性保証のための溶接配管の残留応力推定手法の概念提案 : 第3報(フェロー賞対象ポスターセッション)
スポンサーリンク
概要
- 論文の詳細を見る
To assure structural integrity for operating welded plants, it is required to evaluate welding residual stresses. As a nondestructive method, the bead flush method has been proposed. In this method, residual stresses are calculated by an FEM (Finite Element Method) analysis elastically from eigen-strains that can be estimated in the inverse analysis from release strains in removal of reinforcement of weld. Even if the actual bead height is relatively low and thus the inverse analysis is difficult because of the poor information from the strain gauges, the effectiveness of this method has been proved by attempting qualitative determination of the parameters for stabilization in the inverse analysis. In this study, for further improvement of the estimation reliability, the L-curve method is introduced to determine stabilizing level qualitatively.
- 2010-10-09
著者
関連論文
- 265 応答曲面法を用いたビードフラッシュ法による溶接残留応用の逆問題解析(GS03 積層板・熱応力)
- 2501 リスク解析援用型構造健全性保証のための溶接配管の残留応力推定手法の概念提案(S29-1 原子力発電(1),21世紀地球環境革命の機械工学:人・マイクロナノ・エネルギー・環境)
- P70 デザインバイアナリシスのための溶接固有ひずみの逆解析手法とその影響因子評価(シミュレーション,ポスター講演3)
- PS10 リスク解析援用型構造健全性保証のための溶接配管の残留応力推定手法の概念提案(第2報)(ポスターセッション)
- 201 余盛り除去による溶接残留応力の非破壊評価手法の実験的検証
- 403 解析に基づく設計・維持管理のための画像解析による溶接変形・残留応力評価手法の概念提案 : 第2報,シミュレーションによる実証(GS-11 溶接3)
- 3912 溶接変形・残留応力の逆解析手法のための画像撮影技法の研究 : 第1報 ボケ画像の採用(S17-2 光学的手法,S17 実験力学における最近の展開)
- 812 腐食環境下における純銅の遅れ破壊の発生に関する MD 解析
- 2503 画像処理に基づく溶接変形・残留応力の逆問題解析のための実画像解析精度向上に関する研究(S29-1 原子力発電(1),21世紀地球環境革命の機械工学:人・マイクロナノ・エネルギー・環境)
- K0304 安全・安心へのパラダイムシフトを読み解く(基調講演)
- 402 解析に基づく設計・維持管理のための画像解析による溶接変形・残留応力評価手法の概念提案 : 第1報 手法の定式化(GS-11 溶接3)
- A533B-1鋼の弾塑性破壊抵抗に及ぼす試験片採取方位の影響 (「フラクトグラフィと事故解析」特集号)
- PS34 デザインバイアナリシスのための溶接固有ひずみ逆解析手法とその影響因子評価 : 第5報(ポスターセッション)
- PS01 リスク解析援用型構造健全性保証のための溶接配管の残留応力推定手法の概念提案(ポスターセッション)
- 208 連続余盛り除去による溶接配管へのビードフラッシュ法の適用精度向上(OS6-1 非破壊評価と構造モニタリング,OS6 非破壊評価と構造モニタリング)
- PS53 リスク解析援用型構造健全性保証のための溶接配管の残留応力推定手法の概念提案 : 第3報(フェロー賞対象ポスターセッション)