306 しゃ熱コーティング材のトップコートヤング率および気孔率に及ぼす高温曝露の影響(OS3-2 薄膜・コーティング材の機械的特性と界面強度特性)
スポンサーリンク
概要
- 論文の詳細を見る
In this study, 8wt% Yttria Stabilized Zirconia (8YSZ) specimens prepared by air plasma spraying were subjected to high temperature exposure at 1000℃ or 1200℃. After exposure, instrumented indentation test was carried out to evaluate their Young's modulus. In addition, measurements of porosity by using Mercury Intrusion Porosimetry or using Optical Interferometric Profiler were conducted at the same time. Change behavior and mechanism of their Young's modulus was discussed. As the result, it was seen that sintering phenomena of 1000℃ was only progressed at imperfect contact region between splats, therefore, Young's modulus initially increased and change of their porosity was little. This fact suggests necessity of new procedure that is high resolution to detect micro areal change.
- 一般社団法人日本機械学会の論文
- 2010-10-09
著者
関連論文
- シート座面強度とシートベルト損傷との関係
- 押込み試験方式を利用したしゃ熱コーティング材のヤング率測定法
- P-13 教育GP「つもり学習からの脱却」 : 材料系の実施報告(ポスター発表,(08)工学教育に関するGood Practice)
- 4-325 教育GP「つもり学習からの脱却」 : 材料系における「工学リテラシー入門」の実施報告((08)工学教育に関するGood Practice-III,口頭発表論文)
- プラズマ溶射セラミックコーティング材の熱サイクル損傷特性に関する研究
- 傾斜組成しゃ熱コーティングの熱サイクル損傷機構
- 217 HOT-DIPすずめっき材の中間合金層成長とめっき密着性に及ぼす熱処理条件の影響(金属/金属基複合材料(2),ものづくりにおける基礎研究と先端技術の融合)
- 216 HOT-DIPすずめっき材の曲げ試験による損傷評価法(金属/金属基複合材料(2),ものづくりにおける基礎研究と先端技術の融合)
- 120 しゃ熱コーティング材のトップコートヤング率に及ぼす高温曝露の影響(コーティング・溶射・薄膜プロセス(2),ものづくりにおける基礎研究と先端技術の融合)
- 306 しゃ熱コーティング材のトップコートヤング率および気孔率に及ぼす高温曝露の影響(OS3-2 薄膜・コーティング材の機械的特性と界面強度特性)
- 218 W系金属化合物薄膜の拡散熱処理による形成および機械的特性評価(金属/金属基複合材料(3),ものづくりにおける基礎研究と先端技術の融合)
- 119 しゃ熱コーティング材の熱伝導率及び気孔率におよぼす高温曝露の影響(コーティング・溶射・薄膜プロセス(2),ものづくりにおける基礎研究と先端技術の融合)
- 衝突実験によるシート座面変形とシートベルト損傷に関する研究 : シート座面強度に関する安全基準の提案
- 224 プラズマ溶射HApコーティング材の密着強度評価(生体・医療材料I,生体・医療材料,オーガナイスドセッション10)
- インデンテーション法による溶射皮膜の機械的特性評価