We performed size-dependent nickel plating of a tapered fiber under 1MHz ultrasonic irradiation using two plating units with different water depths of 8 cm and 23 cm. The two obtained probes have nickel thickness profiles which gradually decrease from the foot of the tapered core toward the tip. However, we could not uniformly plated the whole flat end of the clad with nickel by the unit with a smaller water depth of 8 cm.