413 ボイラ用ステンレス用鋼の熱疲労挙動(OS4(1) エネルギー・環境負荷低減機器・材料の強度)
スポンサーリンク
概要
- 論文の詳細を見る
Thermal fatigue tests were conducted for austenitic stainless steel, SUS310S for boiler. The higher the heating temperature the smaller the number of heat cycles for thermal fatigue crack initiation is. The higher the heating temperature the faster the crack propagation rate is. The thermal fatigue crack propagation rate of SUS310S steel was slower than that of SB410 steel. Striation was predominantly observed on fracture surfaces of SUS310S steel. The striation spacing per cycle, S obtained from the measured striation spacing ⊿S versus ⊿K curve was well coincident with the da/dN〜⊿K curve in relatively higher ⊿K region at all heated temperature. It can be concluded that thermal fatigue crack of boiler steel SUS310S propagate in association with striation.
- 一般社団法人日本機械学会の論文
- 2006-08-03
著者
関連論文
- セラミック溶射を施した構造用鋼の熱サイクル破損特性に及ぼすボンドコート厚さの影響
- ジルコニア溶射を施した構造用鋼の熱サイクルおよび熱衝撃破損特性
- 219 ジルコニアコーティング材の耐熱特性(高温強度)
- 316 セラミックコーティング材の耐熱特性に関する検討
- 314 熱サイクルをうけたセラミックコーティング材の破損特性
- OS0705 粉末高速度鋼のギガサイクル疲労挙動(構造用材料の疲労挙動と寿命評価,オーガナイズドセッション)
- 1254 冷間鍛造金型用鋼の破壊挙動(G03-9 材料力学(9)疲労・強度2,21世紀地球環境革命の機械工学:人・マイクロナノ・エネルギー・環境)
- 第54回材料と環境討論会報告
- 618 冷間鍛造金型用鋼のギガサイクル疲労挙動(高サイクル疲労I,オーガナイズドセッション1.疲労の計測・解析・評価)
- K4 蒸気タービン動翼用12Crステンレス鋼の腐食疲労挙動(OS4 エネルギー・環境負荷低減機器・材料の強度)
- 405 非破壊検査による長期使用したSS41鋼溶接継手の破壊靭性(OS3-1 非破壊検査,OS3 エネルギー構造機器の健全性評価と信頼性の高度化3)
- 3611 長期使用した構造物における腐食鋼材の残存強度評価(S13-3 環境効果,S13 実用構造材料の疲労問題と健全性評価)
- 長期使用したSS41鋼および溶接継手の破壊靭性(技術OS2-3 経年劣化,技術OS2 電力設備の健全性)
- 307 ステンレス鋼の腐食疲労き裂発生挙動(疲労に及ぼす環境の影響I,疲労における機構と評価,オーガナイスドセッション1)
- 413 ボイラ用ステンレス用鋼の熱疲労挙動(OS4(1) エネルギー・環境負荷低減機器・材料の強度)
- 111 ボイラ用鋼の熱疲労挙動(実働荷重と熱疲労,疲労の機構と強度信頼性,オーガナイスドセッション1,第53期学術講演会)
- 725 ボイラ用鋼の熱疲労挙動
- 1120 高強度オーステナイト系ステンレス鋼の超音波腐食疲労挙動(OS11-5 材料の疲労挙動と損傷評価-環境-)
- 冷間鍛造金型の破損解析におけるミクロフラクトグラフィの役割
- 117 低合金鋼の腐食疲労強度におよぼす窒化の影響(表面処理,疲労挙動と予寿命評価,オーガナイスドセッション1)
- 506 高速度鋼切欠き試験片のギガサイクル疲労挙動(超高サイクル疲労I,疲労研究の課題と展望,オーガナイスドセッション1)
- 719 冷間鍛造金型用鋼の高サイクル疲労挙動(疲労挙動とメカニズム,疲労損傷の機構解明と評価,オーガナイスドセッション1)