56 血液接着剤に関する研究(第VI報) : 全血液接着剤の熱圧試験に就いて(1)
スポンサーリンク
概要
- 論文の詳細を見る
1. This paper deals with the factors related to gluing strength of whole blood glue by hot press.2. When a small amount of alkali (especially NaOH or Ca(OH)) is added to the whole blood glue material, stronger gluing strength can obtain.3.In order to make plywood with 3 phis of rotary-cut veneers of birch, each having the thickness of 1.5 mm, the following conditions are necessary. The time of pressing : 12-15 minutes, the temperature of gluing : 110-120℃, joining pressure : about 15 kg/cm^2,the amount of glue spread : 0.02-0.025 g/cm^2 (one face).4. When the glue mixture is prepared from the dry whole blood glue material and water, it is preferable that the proportion of water to the glue material should be within 2 in weight.5. When the amount of alkali addition is reasonable, the working life of this glue mixture is fairly long.And the maximum gluing strength can obtain in a few hours after the glue mixed.6. When pressure is applied 20-40 minutes later after a rechipt glue mixture is spread on the veneer, better result can obtain.
- 一般社団法人日本森林学会の論文
- 1952-10-25
著者
関連論文
- 血液接着剤に関する研究(第10報) : 血液の成分による接着強度の差異について
- 血液接着剤に関する研究 (第8報) : 血餠接着剤について(1)
- 411.血液接着剤に関する研究(第IX報) : 血餅接着剤の熱圧温度と圧締力が接着強度に及ぼす影響について(第65回日本林学会大会)
- 血液接着剤に関する研究(第VII報) : 全血液接着剤の熱圧試験について(2)
- 56 血液接着剤に関する研究(第VI報) : 全血液接着剤の熱圧試験に就いて(1)
- 30 血液接着剤に関する研究 (第4報) : 血漿接着剤の熱圧試験に就いて (1)
- 血液接着剤に関する研究(第4報) : 血漿接着剤の熱圧試験に就いて(1)(林産の部)(第60回日本林學會大會並に第5回九州支部大會)
- 51 血液接着剤に関する研究(第2報) : 脱繊血接着剤の熱圧試験に就て