For the investigation of fracture criteria, adhesive tensile strengths of scarf and butt joints bonded by a brittle and two ductile epoxy adhesives have been measured and three-dimensional finite element analyses have been performed. Deformation of the joints influenced considerable by mechanical properties of adhesives. Fracture of the joints bonded by the brittle adhesive obeyed maximum principal stress criterion. In the scarf angles of 15゜ to 60゜, fracture of the joints bonded by the ductile adhesives obeyed von Mises criterion and in the scarf angles more than 60゜, brittle (cleavage) fracture occured for those joints by plastic constraint due to increase of stress triaxiallity in adhesive layers. Locations of fracture initiation and fracture modes of adhesive layers observed with an optical microscope and a a scanning electron microscope agreed with those expected from experimental results of deformation and adhesive tensile strength, and results of stress analyses.
- 一般社団法人日本機械学会の論文
- 1985-03-25
著者
関連論文
- 2008年度色材研究発表会参加記
- 引張り荷重を受ける単純重ね合せ接着継手の弾塑性有限要素応力解析と強度
- 引張せん断荷重を受ける二重重ね合わせ接着継手の弾塑性有限要素解析と強度について
- 引張せん断荷重を受ける単純重ね合わせ接着継手の弾塑性有限要素解析
- ステンレス鋼重ね合せ接着継手の湿潤・応力負荷条件下の耐久性
- ステンレス鋼接着継手の湿潤・応力下の耐久性(第2報)
- ステンレス鋼接着継手の湿潤・応力下の耐久性
- 車両製造にみる機能接着・構造接着(製造にみる接着接合技術)
- 3軸応力下における接着層の降伏および破壊挙動
- 多軸応力下における分散系接着剤の破壊及び降伏挙動
- 車両における接着剤の適用例と動向
- 引張りせん断荷重を受ける二重重ね合せ接着継手の被着体材料特性が継手強度に及ぼす影響
- 628 多軸応力下におけるゴム変成エポキシ接着剤の降伏挙動
- 411 ゴム変成接着剤の多軸応力下における降伏挙動
- 組合せ応力下の接着継手の応力状態および破壊と接着剤の力学的性質との関係
- 鉄道車両
- 車両における構造接着技術の現状と将来
- 鋼のスカーフおよびバット継手の引張接着強度 : 第3報,接着層の厚さと接着強度との関係
- 鋼のスカーフおよびバット継手の引張接着強度 : 第2報, 接着剤の力学的性質と継手の破壊条件との関係
- 鋼のスカーフ接着継手の曲げ応力および接着層収縮応力の有限要素解析
- 鋼のスカーフおよびバット継手の引張接着強度 : 第1報,ぜい性接着剤の場合
- 引張りを受ける鋼のスカーフ接着継手の三次元有限要素解析