Torsional and tensile tests of alumina and silicon carbide fibers from precursors were carried out. Their shear moduli, torsional strengths, Young's moduli and tensile strengths were evaluated and compared. Their shear moduli are about one half of their Young's moduli. Their fracture surfaces show the characteristic feature of isotropic brittle structure. The measured torsional strength of the alumina fiber coincides with that deduced from the tensile strength. Thus, this fiber has extremely isotropic properties of not only structure and moduli but also of strength. However, the measured torsional strength of the silicon carbide fiber is weaker than that deduced from the tensile strength. As for this reason, it is supposed that the sheath is weaker than the core and/or defects are preferentially oriented to the fiber axis.
- 一般社団法人日本機械学会の論文
- 1991-03-25
著者
関連論文
- 複合材料の設計と評価の最前線 : 2.繊維と界面の評価法
- 303 CFRPにおける界面の接着強度と炭素繊維の表面特性の関係(複合材料I)
- ILSSの時間 : 温度依存性に及ぼすCFRP中炭素繊維表面の影響
- 205 炭素繊維の直角方向圧縮試験(PMC:強度とき裂)
- 各種CFRPの高温3点曲げショートビーム法強度とその破壊モード(高分子系複合材料)
- 800kg/cm^2の加圧水中浸せきによるCFRPとGFRPの劣化
- CFRP,GFRPの水中劣化に及ぼす水圧の影響
- ミクロコンポジットを用いたC/Cの界面せん断強度の測定
- ミクロコンポジット引き抜き試験
- 338 SiCウィスカー強化アルミニウム合金のウィスカー含有量評価法(セラミックスI)
- Advanced Composites'93に参加して
- 夢の超耐熱材料を目指して
- Achievement in Composites in Japan and the United States, Akira KOBAYASHI(編), 1990年, 古今書院発行, 23.4×16.0 cm, 708ページ, 28000円
- 等方性セラミック繊維のねじりおよび引張特性
- 339 無機繊維のねじり試験と引張試験(セラミックスI)
- ミクロコンポジット試験による繰り返し荷重下での界面強度評価の検討
- イミド系樹脂による炭素繊維/炭素マトリックスの界面制御
- 一方向強化CFRPの90℃引張り破面
- 各種被覆炭素繊維のアルミニウムに対する適合性
- 繊維強化金属の繊維含有率の評価法
- 習字で使う墨はどのようにしてつくるのですか?
- "接合材料入門", 宮入裕未(著), (1997年, 裳華房発行, A5判, 243ページ, 本体3600円)
- "ウッドセラミックス", 岡部敏弘(監修), 齋藤幸司, 堀切川一男, 大塚正久, 伏見賢美(編), (1996年, 内田老鶴圃, B5判, 269ページ, 定価4944円)
- "つくる立場からみた 複合材料入門", 大谷 杉郎(著), 1995年, 裳華房発行, B5判, 189ページ, 定価2884円
- 一方向強化CFRPの90℃引張り強度と炭素繊維の表面特性との関係