MgSiO_3の加熱特性について : ステアタイトの劣化現象に関する研究 (第2報)
スポンサーリンク
概要
- 論文の詳細を見る
In the literature concerning the deterioration of steatite (H. Thurnaure, A. R. Rodriguez, J. Am. Ceram. Soc., 25, 443 (1942); W. R. Foster, J. Am. Ceram. Soc., 34, 255 (1951)) the growth of magnesium metasilicate formed in the body, or the transformation of protoenstatite comming out in the cooling period were said as the principal sources of this defect. However, there is no example of discussing in detail on the influence of glass phase coexisting in the body.The author has carried out the investigations on the characteristic properties of MgSiO3 with and without glass phase in high temperatures using X-ray diffraction, differential thermal analysis, dilatmetric method and electron microscope. The MgSiO3 without glass phase showed the same characteristicsof transformation as pointed out by W. R. Foster (l. c.), while the MgSiO3 with glass phase (protoenstatite), when quenched in some degree, was readily super cooled to secure the stability at an ordinary temperature.Based on his experimental results the author discussed the deterioration of steatite pointing out that the devitrification in glass or liquid phase caused by the shift of phase equilibrium in the body in the cooling period plays the leading roll in this phenomenon.
- 社団法人日本セラミックス協会の論文
- 1959-07-01
著者
関連論文
- MgO-BaO-Al_2O_3-SiO_2系平衡図とステアクタイトの劣化現象との関連性について : ステアタイトの劣化現象に関する研究 (第4報)
- BsSi_2O_5-Mg_2SiO_4-SiO_2系平衡図について : ステアタイトの劣化現象に関する研究 (第3報)
- MgSiO_3の加熱特性について : ステアタイトの劣化現象に関する研究 (第2報)
- 劣化したステアタイトの過熱異状伸縮特性とその化学組成について : ステアタイトの劣化現象に関する研究 (第1報)