This paper examines the strain controlled fatigue-creep interaction (FCI) life of directionally solidified (DS) superalloy Rene 80H. The author previously proposed a frequency-modified total strain energy parameter, obtained from the total tensile strain energy and tensile loading time, for use in evaluating the failure life of equiaxial Ni and Co based superalloys under FCI conditions. The present paper examines the applicability of this parameter for predicting the FCI life of DS Rene 80H. The FCI life prediction by the total strain range was first evaluated. It was found that the FCI life of the specimens cut in parallel to the DS direction of a directionally solidified plate was longer than that of the specimens cut in transverse to the DS direction. In addition, the specimen life under tensile hold time conditions was longer than under compressive hold time conditions. The FCI life prediction by the frequency-modified total strain energy parameter was evaluated next. For the specimens in both directions, there is a linear correlation between this parameter and the cycles to failure. Therefore, it is concluded that the FCI life prediction for DS Rene 80H can be made by using this parameter.
- 1993-01-15
著者
関連論文
- 全ひずみエネルギに基づくCo基鋳造耐熱合金の疲労・クリープ相互作用下の寿命評価
- NiおよびCo基鋳造合金の高温低サイクル疲労強度と静的強度の温度依存性の相関について
- Ni基超合金Ren880の疲労・クリープ相互作用下の寿命に及ぼす耐食コーティングの影響
- 圧縮残留応力のあるロータディスクの脆性破壊強度
- B-1 圧縮残留応力のあるロータディスクの脆性破壊強度
- 一方向凝固鋳造超合金Rene 80Hの全ひずみエネルギに基づく疲労・クリープ相互作用下の寿命評価
- 高耐力耐熱合金の疲労・クリープ相互作用下におけるき裂進展に基づく寿命評価法の検討
- Rene80 Ni基超合金の疲労・クリープ寿命とクリープ強度の全ひずみエネルギに基づく相関性の検討
- 高耐力熱合金に対する全ひずみエネルギーに基づく疲労・クリープ相互作用下の寿命予測法の提案
- IN738CL の高温低サイクル疲労と熱疲労下における微小き裂発生, 進展挙動
- 240 重回帰分析による超耐熱合金の高温低サイクル疲労と静的強度の相関性の検討(高温強度)
- Ni基単結晶超合金の引張・圧縮‐繰返しねじり負荷での多軸低サイクル疲労寿命評価