鋼質の缺陷としての水素脆性の重要性に就て
スポンサーリンク
概要
- 論文の詳細を見る
The hydrogen contained in ingots vanishes usually during the course of forging and heat-treatment. The hydrogen of about 0.5 c.c. per 100 grams may some times remain in the forged material after the heat-treatment due to various reasons, which may cause the hydrogen-brittleness In this paper, the author points out that this kind of hydrogen-brittleness is not less influential than the sand and ghost brittleness in hurting the toughness of steel, and explans with actual examples that the defect in often mistaken as the seasoning phenomenon from its properties or is liable to be overlooked under the covering of the mass effect. He also describes, that the hydrogen-brittless facilitates the generation of flakes, in accordance with the results of the experimental generation of flakes, and emphasizes that the encouragement of gradual cooling after forging signifies a great importancy in ivew of the hydrogen-brittleness.
- 社団法人日本鉄鋼協会の論文
- 1938-11-25
著者
関連論文
- 442 二相組織のステンレス鋼の熱処理に関する研究 : 第 6 報分配係数および Cr, Ni 当量(ステンレス鋼, 性質, 日本鉄鋼協会 第 97 回(春季)講演大会)
- 284 2 段時効硬化について : 二相組織のステンレス鋼の熱処理に関する研究 IV(耐酸化ステンレス鋼・ステンレス鋼の諸性質, 性質, 日本鉄鋼協会第 90 回(秋季)講演大会)
- 169 Strain Aging について : 二相組織のステンレス鋼の熱処理に関する研究第 3 報(工具鋼・その他, 加工・性質・分析・検査・計測, 日本鉄鋼協会第 84 回(秋季)講演大会)
- 引張試驗片に生ずる星形破面に就て
- 合金鋼に現はれる特殊の時効現象に就て
- 鋼の剪斷力に就て
- 鋼に含まれる珪素に關する研究 : (IV) 低炭素 Si Mn Cr 鋼に就て
- 鋼に含まれる珪素に關する研究 : (III) 時効性強靱珪素鋼に就て
- 鋼に含まれる珪素に關する研究 (II) : フエライトの材力に及ぼす珪素の影響に就て
- 鋼質の缺陷としての水素脆性の重要性に就て
- Ni-Cr 鋼の應力歪圖に及ぼす熱處理の影響