Ni-Cr 鋼の應力歪圖に及ぼす熱處理の影響
スポンサーリンク
概要
- 論文の詳細を見る
The author made various heat-treatments on Ni-Cr steel (0.3% C, 3.3% Ni and 0.8% Cr), and investigated the influence of heat-treatment on the form of stress-strain diagram in the vicinity of yielding point and the degree of work-hardening (or the difference between the tensile strength and the yielding point) by accurately measuring the stress-strain diagram up to 5% strain. The results of the investigation are outlined below : - A. Investigation by quenching and tempering (1) When the tempering temperature is raised to about 40℃ below Ac_1 (715℃), carbide begins to aggregate in crystallographic planes, and simultaneously the form of the stress-strain diagram varies and the yielding point lowers ; contrarily the degree of work-hardening suddenly increases. (2) When the tempering temperature approaches Ac_1, the aggregated carbide makes beautiful laminar layers forming a special structure which is named "laminar sorbite" by the author, and the yielding point steadily lowers, whilst the degree of work-hardening considerably increases. (3) In accordance with the reduction of the cooling speed in quenching, the yielding point lowers, but the degree of work-hardening contrarily increases, whilst the cooling speed in tempering has no effect. B. Investigation by double quenching. (1) Double quenching is a heat treatment, in which the secondary quenching is carried out between the stages of the primary quenching and the tempering. In accordance with the temperature of the secondary quenching, two kinds of completely different mechanical properties are given to the material. (2) When the secondary quenching temperature is in the vicinity of Ac_1, i. e., 680°-730℃, the structure is of laminar sorbite with a low yielding point and a condiderably high degree of workhardening. (3) When the secondary quenching temperature is below Ac_3 (775℃), i. e., 740°-770℃, a special structure named "granular pearlite" by the author appears, and the yielding continues over 2% and the yielding point is comparatively high but the degree of work-hardening is extremely small.
- 社団法人日本鉄鋼協会の論文
- 1937-12-25
著者
関連論文
- 442 二相組織のステンレス鋼の熱処理に関する研究 : 第 6 報分配係数および Cr, Ni 当量(ステンレス鋼, 性質, 日本鉄鋼協会 第 97 回(春季)講演大会)
- 284 2 段時効硬化について : 二相組織のステンレス鋼の熱処理に関する研究 IV(耐酸化ステンレス鋼・ステンレス鋼の諸性質, 性質, 日本鉄鋼協会第 90 回(秋季)講演大会)
- 169 Strain Aging について : 二相組織のステンレス鋼の熱処理に関する研究第 3 報(工具鋼・その他, 加工・性質・分析・検査・計測, 日本鉄鋼協会第 84 回(秋季)講演大会)
- 引張試驗片に生ずる星形破面に就て
- 合金鋼に現はれる特殊の時効現象に就て
- 鋼の剪斷力に就て
- 鋼に含まれる珪素に關する研究 : (IV) 低炭素 Si Mn Cr 鋼に就て
- 鋼に含まれる珪素に關する研究 : (III) 時効性強靱珪素鋼に就て
- 鋼に含まれる珪素に關する研究 (II) : フエライトの材力に及ぼす珪素の影響に就て
- 鋼質の缺陷としての水素脆性の重要性に就て
- Ni-Cr 鋼の應力歪圖に及ぼす熱處理の影響