Deoxidation of liquid iron with barium was studied in the temperature range from 1600 to 1700℃. Barium and oxygen dissolved in liquid iron were brought into equilibrium in presence of pure barium oxide in the lime crucible under the inert gas atmosphere of argon. The equilibrium constant and standard free energy of the deoxidation reaction "BaO(s)=<Ba>___-(%)+O__-(%)" were obtained as follows : logK=-9980/T-1.82 (±0.11) △G°=191000+34.9T(J) (±4 kJ) The temperature dependences of the interaction parameters were expressed by the following equations : e^<Ba>_O=27.1-1.48×10^5/T e^O_<Ba>=233-1.27×10^6/T The standard free energy of solution of barium in liquid iron and the activity coefficient of barium in the infinite dilute liquid iron solution refered to pure barium (γ°_<Ba>) were calculated and discussed.
- 社団法人日本鉄鋼協会の論文
- 1992-02-01
著者
-
萬谷 志郎
東北大学工学部
-
井口 泰孝
東北大学工学部
-
井口 〓孝
Department Of Materials Processing Tohoku University
-
加藤 周一
東北大学大学院:(現)(株)神戸製鋼所 (社)日本鉄鋼連盟
関連論文
- 100 溶鉄中の硫黄の活量について
- 100 溶鉄中の硫黄の活量について(製鋼, 日本鉄鋼協会第 72 回(秋季)講演大会講演)
- ラマン分光法による CaO-MeO-SiO_2, MnO-SiO_2 および FeO-SiO_2 系スラグの構造研究
- 高炉スラグ中のガスの挙動
- 溶鉄の窒素溶解度におよぼす C, Al, Si, P, Mn および Ni の影響
- 溶鉄の窒素溶解度および窒素溶解度におよぼす VI_a 族元素の影響
- 高温熱量計による鉄合金の混合熱の測定
- 108 ラマン分光法による MnO-SiO_2, FeO-SiO_2 および CaO-MeO-SiO_2 系スラグの構造研究(精錬基礎, 製鋼, 日本鉄鋼協会 第 101 回(春季)講演大会)
- 56 高炉スラグ中のガス成分の定量(製銑スラグ・製銑基礎 (II), 製銑, 日本鉄鋼協会 第 100 回(秋季)講演大会)
- 高周波攪拌浴における珪素による溶鋼の脱酸機構