Surface Wettability in Terms of the Height and Depression of Diverse Microstructures and Their Sizes
スポンサーリンク
概要
- 論文の詳細を見る
Surface wettability in terms of the height, depression, and sizes of diverse microstructures was examined. We considered three different types of microstructures: square pillars, square pores, and hexagonal pores. An increase in pore fraction causes a decrease in the contact area between a water drop and the microstructures, resulting in an increase in contact angle. It was verified that the contact angle of the square pillar microstructure is higher than those of the square pore and hexagonal pore microstructures for the same pore fraction. Of the pore-based microstructures, the square-pore microstructure has a higher contact angle than the hexagonal pore microstructure. However, it was observed that water drops were more stable with respect to pore fraction on the hexagonal pore microstructures. In addition, compared with the pillar microstructure, the pore-based microstructures exhibited more stable contact angles for different structure heights.
- 2009-09-25
著者
-
Lee Sang
Graduate School Engineering Yokohama National Univ.
-
Lee Sang
Graduate School of Mechanical Engineering, Pusan National University, Jangjeon-dong, Geumjeong-gu, Busan 609-735, Korea
-
Park Chi
Graduate School of Mechanical Engineering, Pusan National University, Jangjeon-dong, Geumjeong-gu, Busan 609-735, Korea
-
Bae Seung
Graduate School of Mechanical Engineering, Pusan National University, Jangjeon-dong, Geumjeong-gu, Busan 609-735, Korea
-
Go Jeung
Graduate School of Mechanical Engineering, Pusan National University, Jangjeon-dong, Geumjeong-gu, Busan 609-735, Korea
-
Shin Bosung
ERC/NSDM, Pusan National University, Jangjeon-dong, Geumjeong-gu, Busan 609-735, Korea
-
Ko Jong
Graduate School of Mechanical Engineering, Pusan National University, Jangjeon-dong, Geumjeong-gu, Busan 609-735, Korea
関連論文
- OS8(3)-12(OS08W0124) High Temperature and Fatigue Strength of Crack-Healed Silicon Carbide Ceramics
- A Glycosidic Spinasterol from Koreana stewartia Promotes Procollagen Production and Inhibits Matrix Metalloproteinase-1 Expression in UVB-Irradiated Human Dermal Fibroblasts
- Surface Wettability in Terms of the Height and Depression of Diverse Microstructures and Their Sizes