In vitro evaluation of marginal and internal adaptation of three-unit fixed dental prostheses produced by stereolithography
スポンサーリンク
概要
- 論文の詳細を見る
The purpose of this study was to investigate, by measuring the gap, the possible clinical use of three-unit fixed dental prostheses (FDPs) manufactured using stereolithography. A total of 20 epoxy models were built with a same case (abutment teeth 14, 16). The 40 specimens were produced using the stereolithography (SLA) and wax-up (LW). The 960 gaps of the 40 specimens produced were measured by a silicone replica. The Wilcoxon rank sum test was then used to compare and analyze the data obtained from the two groups (α=0.05). The total gap, as measured from the SLA and LW groups, was 98.6 and 66.6 µm, respectively. The results indicate that the gap in the SLA group is statistically significantly greater than that in the LW group (p<0.05). Further assessment and improvement of the SLA method for the fabrication of FDPs is evidently still required.
著者
-
KIM Ji-Hwan
Department of Dental Laboratory Science and Engineering Korea University
-
KIM Jae-Hong
Department of Dermatology, Yonsei University Wonju College of Medicine
-
KIM Ki-Baek
Department of Dental Laboratory Science and Engineering, College of Health Science, Korea University
-
KIM Woong-Chul
Department of Dental Laboratory Science and Engineering, College of Health Science, Korea University
関連論文
- Fabrication and characterization of highly porous calcium phosphate (CaP) ceramics by freezing foamed aqueous CaP suspensions
- Activation of Smooth Muscel α-Actin Promoter in ras-Transformed Cells by Treatments with Antimitotic Agents: Correlation with Stimulation of SRF: SRE Mediated Gene Transcription
- Variant of phacomatosis pigmentokeratotica
- In vitro evaluation of marginal and internal adaptation of three-unit fixed dental prostheses produced by stereolithography