ABSTRACTAn experimental study for obtaining a high performance ceramics of titanium diboride and tungsten carbide composites (TBWC) are described. WC content 10 to 90 volume percent tungsten was examined. The TBWC is inexpensive and can be fabricated by a hotpress-sintering process. The TBWC with density 95 % and above of the theoretical value were obtained using constituent powder of micron size by hotpress sintering. The TBWC thus obtained consists of four phases which are (Ti, W)B2, (W, Ti)C and 2 types of (W, Ti)B. Unlike porycrystalline diamond and cBN compacts, in which the intrinsic hardness or strength of the constituents is utilized, it seems that the TBWC is basically hardened or strengthend by solution hardening or dispersion strengthening mechanisms. Those mechanisms were confirmed by metallography, X-ray diffraction, electron probe microanalysis and mechanical tests.
- 一般社団法人 粉体粉末冶金協会の論文
著者
関連論文
- ネオジム・イットリウム-ニオビウム系酸化物の擬弾性挙動と微小塑性
- 粉体押出成形によるMg-Zr合金の創製と機械的特性
- 粉体押出成形によるマグネシウム合金の機械的特性の改善
- 高温高圧下で使用される金属被膜形成グリース
- 129 高Si-Al系軸受合金の機械的特性(摩擦・摩耗材料(2),ものづくりにおける基礎研究と先端技術の融合)
- TiB2–WC 系複合セラミックスの創製と機械的性質