This report discusses the cast hemispherical core dies for the hot extrusion of the hollow shaped aluminum alloys. The hemispherical core die is casted in SKD 61. The end face of the core of this die is hemispherical on the entry side of the billet. The maximum tensile stress appearing around the root of a mandrel of the core is remarkably reduced in comparison with a port-hole die, which results in suppresion of crack initiation. The solidification simulation was used for the purpose of predicting the solidification defects and increasing the temperature gradient at the point of tensile stress. The hemispherical cast dies with the temperature gradient of more than 303 K/cm had the same high-temperature stress characteristics (according to the tensile test piece, which is cut from the cast die) and demonstrated the same extrusion features as that of forged hemispherical core dies. By using this type of cast hemispherical core die, the raw material weight is 38.3 % of a forged hemispherical core die. Moreover, the die forming time is shortened by 50 %.
- Japan Foundry Engineering Societyの論文
Japan Foundry Engineering Society | 論文
- 球状黒鉛鋳鉄の延性破壊に及ぼす応力3軸度及び基地組織の影響
- 紡織機鋳物の鋳造法に就いて (其の一)
- 光ファイバで紫外線を導光した光造型機の開発と石こう鋳造への適用
- 薄肉球状黒鉛鋳鉄の黒鉛粒数に及ぼす元湯硫黄量,冷却速度及び希土類元素添加時期の影響
- Fe-Si合金及びFe-C-Si合金の塩浴窒化に及ぼすSiの影響とFe,Siの窒化物について