高鉛青銅の凝固時における錫の挙動
スポンサーリンク
概要
- 論文の詳細を見る
The redistributing behaviors of tin in the Cu-20%Pb-2 or 5%Sn bronzes during freezing wered etermined by means of the X-ray microanalysis. Cosiderable release of tin from the alpha solid during freezing results in extreme condensation in the remained liquid as much as 20% at the end of the monotectic reaction. The ratios tin concentration in the solid to that in the liquid are 0·08 to 0.13 and 0.14 to 0.20 respectively in the Cu-20%Pb-2 and 5%Sn bronzes and are the least at the initial stage of nucleation for alpha dendrites. The growing alpha solid is often surrounded with the (L1+L2) liquid. The lead-rich L2 phase which is easily aggregated leads to coarse and irregular distribution of lead. Tin once condensec in the liquid is inversely released from the lead-rich liquid and disolved into the alpha solid accompanying with coring in it. Less condensation of tin in the remained liquid is found in the bronzes containing 2% nickel and silver. 0.5% silicon has an inverse effect.
- Japan Foundry Engineering Societyの論文
Japan Foundry Engineering Society | 論文
- 球状黒鉛鋳鉄の延性破壊に及ぼす応力3軸度及び基地組織の影響
- 紡織機鋳物の鋳造法に就いて (其の一)
- 光ファイバで紫外線を導光した光造型機の開発と石こう鋳造への適用
- 薄肉球状黒鉛鋳鉄の黒鉛粒数に及ぼす元湯硫黄量,冷却速度及び希土類元素添加時期の影響
- Fe-Si合金及びFe-C-Si合金の塩浴窒化に及ぼすSiの影響とFe,Siの窒化物について