Noncontact Measurement of Doping Profile for Bare Silicon.
スポンサーリンク
概要
- 論文の詳細を見る
In this study, we evaluate the doping concentrations of bare silicon wafers by noncontact capacitance-voltage (C-V) measurements. The metal-air-insulator-semiconductor (MAIS) method enables the measurement of C-V characteristics of silicon wafers without oxidation and electrode preparation. This method has the advantage that a doping profile close to the wafer surface can be obtained. In our experiment, epitaxial silicon wafers were used to compare the MAIS method with the conventional MIS method. The experimental results obtained from the two methods showed good agreement. Then, doping profiles of boron-doped Czochralski (CZ) wafers were measured by the MAIS method. The result indicated a significant reduction of the doping concentration near the wafer surface. This observation is attributed to the well-known deactivation of boron with atomic hydrogen which permeated the silicon bulk during the polishing process. This deactivation was recovered by annealing in air at 180<SUP>°</SUP>C for 120 min.
- 公益社団法人 応用物理学会の論文
公益社団法人 応用物理学会 | 論文
- Electron Channelling Effect in an Al–Fe–Cu Quasicrystal
- Construction and Performance of a Large-Aperture Wire-Chamber Spectrometer for Pion Scattering Experiments at KEK
- Effect of Plasma Injection on Cold Wall Type MHD Generator
- Development of Scanning μ-RHEED Microscopy for Imaging Polycrystal Grain Structure in LSI
- Boundary Layer Cooling Effect on Semi-Hot Wall Type MHD Channel