Study on zirconium alloys (2 nd Report):Mechanical properties of binary and some ternary alloys
スポンサーリンク
概要
- 論文の詳細を見る
As the laboratory-scale tungsten electrode argon arc melting furnace, designed by the authors, has been completed in their laboratory, nearly twenty binary zirconium alloys as well as several ternary alloys listed in Table 1 and 2, including zircaloy 2 and 3-B have been melted. They were hot forged at 1000°C and then cold rolled down to 0.2mm thick strips, with an intermediate annealing for 1hr at 700°C except two alloys where the amount of alloying element added was too much to be easily worked.Mechanical properties; hardness, tensile properties and spring limit value, have been mea- sured, the results of with are summarized in Table 4 and 5. Titanium was found to be the most effective element to enhance strength of zirconium, followed by aluminium, molybdenum and tin among the alloys considered.Heat treatment response of those alloys, including aging of α-quenched alloys has also been considered, with microscopic observations under polarized light.
- 一般社団法人 軽金属学会の論文
一般社団法人 軽金属学会 | 論文
- Mechanical and wear properties of SiC whisker/ADC12 aluminum alloy composites fabricated by die casting.
- Joining of aluminum and ceramics.
- タイトル無し
- Undercooling and solidification behavior of fluid clumps of second-poured melt of hypereutectic Al-Si alloy in Duplex Casting process.
- Change in apparent viscosity of stirred slurry during production of semi-solid hypereutectic Al-Si alloy by slurry-melt mixing process.