Upsetting textures in ZK60A magnesium alloy.
スポンサーリンク
概要
- 論文の詳細を見る
Texture measurements were made of upsetting forged disk to 50 and 70% reduction from semi-continuously cast rod and extruded rod of ZK60A alloy having weak [1120] and strong [1010] fiber texture parallel to rod axes respectively. The method of Harris for inverse pole figures of fiber textures was used. To verify if the method is appropriate for measurement of forging texture in magnesium, texture in extruded plate of AZ31 alloy was also measured. Initial textures changed during upsetting gradually to [0001] orientation parallel to upsetting direction, sharpness of these fiber texture being more shape at surface layer on disk than inner layer and at higher reduction. Textures in various location in disk from cast bar were uniform in comparison with that from extruded rod in which upsetting direction are parallel to extrusion direction.
- 一般社団法人 軽金属学会の論文
一般社団法人 軽金属学会 | 論文
- Mechanical and wear properties of SiC whisker/ADC12 aluminum alloy composites fabricated by die casting.
- Joining of aluminum and ceramics.
- タイトル無し
- Undercooling and solidification behavior of fluid clumps of second-poured melt of hypereutectic Al-Si alloy in Duplex Casting process.
- Change in apparent viscosity of stirred slurry during production of semi-solid hypereutectic Al-Si alloy by slurry-melt mixing process.